MIROGARD®
Protection without reflection
MIROGARD® offers less than 1% residual reflection compared to around 8% reflection for float glass. Extremely transparent, it also allows up to 99% light transmission. The glass is dip-coated with nanometer-thin layers of metal oxide that form a powerful defense against abrasion and chemicals, as well as light.
EXPLORE MATERIAL PROPERTIES IN DETAIL