Product Variants of CoralPor® Porous Glasses
CoralPor® Nano-Porous
YOUR ADVANTAGES
- Excellent absorption and separation capabilities due to very large internal surface area and narrow pore size distribution
 - Enabling stable results and efficiency due to ultra-robust, long-lasting material. Properties include:
- Low coefficient of thermal expansion
- High thermal stability
- High chemical resistance against a large variety of different media - Available as a powder or monoliths in various shapes and sizes
 
APPLICATIONS
Examples include:
- As a substrate in synthesis processes e.g. for enzymes
 - Thin layer chromatography
 - Ultra- and microfiltration
 
CoralPor® Macro-Porous
YOUR ADVANTAGES
- Excellent thermal stability depending on base glass
 - Completely inorganic
 - Customized surface treatment upon request
 - CoralPor® Macro-Porous Glasses can be produced:
-With an average pore size between 1–500 μm
-A pore volume of up to 80%
-As sintered monoliths in various shapes and sizes
-As porous microspheres / powders
 
APPLICATIONS
Examples include:
- As a substrate in synthesis prcesses e.g. for bioreactors
 - Microfiltration
 - Carrier for liquids or active substances, such as evaporation units in e-cigarettes or vaporizers
 