Product Variants of SCHOTT® Solar Glass

The cover glass portfolio of SCHOTT® Solar Glass includes three precision-engineered variants that combine high optical transmittance with reliable protection. Each product is optimized for specific application profiles, from space missions and optical solar reflectors to advanced terrestrial photovoltaic systems.
SCHOTT® Solar Glass 0787

SCHOTT® Solar Glass 0787

SCHOTT® Solar Glass 0787 is a highly transparent and ultra-thin protective cover glass for photovoltaic cells and optical solar reflectors. Its composition combines excellent radiation stability and high optical performance, ensuring reliable power generation under harsh environmental conditions.
SCHOTT® Solar Glass 0787

CHARACTERISTICS

Manufactured using SCHOTT’s proprietary down-draw process, SCHOTT® Solar Glass 0787 features an ultra-flat fire-polished surface on both sides. Standard thicknesses range between 0.075 mm and 0.15 mm, but can be as low as 0.03 mm and as high as 1.0 mm. The glass can be toughened for enhanced strength and is cerium-doped to minimize solarization and preserve transmittance after prolonged UV and charged particle exposure.


YOUR ADVANTAGES

  • Acts as a barrier layer, protecting solar cells against damage in high-radiation environments.
  • Provides high transmittance in the VIS and NIR spectral range with stable long-term performance.
  • Available as sheets or cut-to-size substrates tailored to customer designs.
  • Certified according to ECSS-E-ST-20-08C and compliant with RoHS and REACH directives.
SCHOTT® Solar Glass sphere

SCHOTT® Solar Glass sphere

SCHOTT® Solar Glass sphere is a technical glass designed for high transmission and lightweight protection in low-radiation environments. As a commercial off-the-shelf (COTS) product, it offers proven performance for both space and terrestrial photovoltaic applications, combining optical quality with cost-efficient scalability and long-term spectral stability.
SCHOTT® Solar Glass sphere

CHARACTERISTICS

SCHOTT® Solar Glass sphere offers an ultra-flat, fire-polished surface with excellent geometric homogeneity and minimal roughness. Standard thicknesses range from 0.03 mm to 0.15 mm, with formats up to 1.0 mm available on request. Its stable oxide composition maintains transparency over decades of exposure while limiting UV transmittance to protect adhesives and coatings.


YOUR ADVANTAGES

  • Ultra-thin formats down to 0.03 mm for lightweight system integration.
  • Extra large formats on request.
  • Maintains high transmittance with minimal UV impact across long lifetimes.
  • Commercial off-the-shelf (COTS) product with short lead times for high volumes.
SCHOTT® Solar Glass exos

SCHOTT® Solar Glass exos

SCHOTT® Solar Glass exos is the next-generation cover glass for advanced photovoltaic arrays and optical systems requiring maximum durability and UV protection. Designed for use with high-efficiency multijunction solar cells and long-duration missions, it combines superior material stability with high optical performance.
SCHOTT® Solar Glass exos

CHARACTERISTICS

SCHOTT® Solar Glass exos combines outstanding material stability with excellent dimensional precision and optical uniformity. It offers the highest UV absorption within the SCHOTT® Solar Glass family and a CTE of approximately 6.9 × 10⁻⁶ K⁻¹, precisely matched to GaAs-based multi-junction cells. Designed in accordance with ECSS requirements, underscoring its suitability for demanding long-term missions.


YOUR ADVANTAGES

  • Maximum UV cut-off for superior protection of solar-cell adhesives and junctions.
  • Excellent transmittance and stability under prolonged radiation and thermal cycling.
  • Precisely engineered CTE for high compatibility with III–V multijunction solar technologies.
  • Developed in line with ECSS qualification standards to ensure material reliability and consistent performance. (ECSS qualification in progress)

Want to know more? Let's talk!

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

Man in glasses in business office on phone while working on laptop_330x190.jpg

1 Step 1
2
3

*Required field

SCHOTT will only use your data to respond to your inquiry. For more information, please click here.