Product Variants of DURAN®
DURAN® in Jumbo Size
CHARACTERISTICS
Since jumbo-sized DURAN® glass tubing is manufactured using the same direct-draw process as standard DURAN® tubing, it offers the same strength, tight tolerances, chemical and electrical resistance, optical quality, and thermal shock resistance.
YOUR ADVANTAGES
- High quality glass tubing with large outer diameter.
 - Tight tolerances and high mechanical strength.
 
DURATAN®
High scratch resistance and strong light transmission properties also make this variant ideal for external use, and a fine break pattern improves the safety characteristics of the glass as it breaks in a less hazardous way.
YOUR ADVANTAGES
On average 2-3 times higher resistance to tensile stress and mechanical impact compared to DURAN®.
Fine break pattern, similar to tempered safety glass (ESG).