Technical Details of SCHOTT® Solar Glass
Designed to endure space – and beyond
| Geometrical properties | Unit | Value |
|---|---|---|
| Thickness* | mm | 0.150 | 0.125 | 0.100 | 0.075 |
* Other thicknesses on request
| Optical properties | Unit | Value |
|---|---|---|
| Refractive index nd | 1.5080 | |
| Edge wavelength λc (τ = 46 %) at t = 0.100 mm | nm |
332 |
| Thermal properties | Unit | Value |
|---|---|---|
|
Transformation temperature Tg
|
°C | 568 |
| Coefficient of thermal expansion - CTE α(20; 300 °C) | 10-6 K-1 |
8.5 |
| Mechanical properties |
Unit | Value |
|---|---|---|
| Density ρ | g/cm³ | 2.51 |
| Young's modulus E | kN/mm² | 70.0 |
| Poisson's ratio µ | 0.216 |
Spectral transmittance of SCHOTT® Solar Glass 0787


| Geometrical properties | Unit | Value |
|---|---|---|
| Thickness* | mm | 0.150 | 0.100 | 0.070 | 0.030 |
* Other thicknesses on request
| Optical properties | Unit | Value |
|---|---|---|
| Refractive index nd | 1.5231 | |
| Edge wavelength λc (τ = 46 %) at t = 0.100 mm | nm |
308 |
| Thermal properties | Unit | Value |
|---|---|---|
| Transformation temperature Tg | °C | 557 |
| Coefficient of thermal expansion – CTE α(20; 300 °C) | 10-6 K-1 | 7.2 |
| Mechanical properties |
Unit | Value |
|---|---|---|
| Density ρ | g/cm³ | 2.51 |
| Young's modulus E | kN/mm² | 72.9 |
| Poisson's ratio µ | 0.21 |
Spectral transmittance of SCHOTT® Solar Glass sphere
| Geometrical properties | Unit | Value |
|---|---|---|
| Thickness* | mm | 0.150 | 0.100 | 0.050 |
* Other thicknesses on request
| Optical properties | Unit | Value |
|---|---|---|
| Refractive index nd | 1.5145 | |
| Edge wavelength λc (τ = 46 %) at t = 0.100 mm | nm |
344 |
| Thermal properties | Unit | Value |
|---|---|---|
| Transformation temperature Tg | °C | 557 |
| Coefficient of thermal expansion – CTE α(20; 300 °C) | in 10 K-1 | 6.9 |
| Mechanical properties |
Unit | Value |
|---|---|---|
| Density ρ | g/cm³ | 2.54 |
| Young's modulus E | kN/mm² | 74.5 |
| Poisson's ratio µ | 0.218 |
Spectral transmittance of SCHOTT® Solar Glass exos
SCHOTT® Solar Glass is available as:
- Sheets
- Cut-to-size substrates
- AR-coated substrates
To find out more, please see the related products on the overview page.