NARIMA®
As a dichroic glass, NARIMA® reflects certain colors while allowing their complementary to be transmitted, depending on the angle of vision. NARIMA® also possesses high scratch resistance and chemical resistance.
Product range
NARIMA® Color Effect Glass is available in the following six variants:
Color Effect Glass | Color changeover of coating (reflection)1 | Color appearance (transmittance) |
---|---|---|
Blue-Gold3 | gold | blue |
Blue-Green2 | violet | blue-green |
Green3 | violet | light-green |
May-Green2 | violet | green |
Yellow3 | blue | yellow |
Orange3 | blue-silver | orange |
1 color reflection depends on the observation angle
2 only available as non-tempered glass
3 can be thermally tempered
Blue-Gold |
Blue-Green |
Green |
May-Green |
Orange |
Yellow |
Standard NARIMA® dimensions and thicknesses
Standard sheet dimension net
- 3,770 mm x 1,700 mm
- 3,180 mm x 1,700 mm
- 1,700 mm x 1,220 mm
Standard thickness
- 4 mm as well as 6 mm with a float glass base available
- 5 mm, 8 mm, 10 mm, 12 mm upon request
NARIMA® has a range of processing options and can be manufactured to create the following forms:
- Laminated glass
- Thermally toughened safety glass
- Insulating glass
- Insulating glass with sun protection and sound insulation
Functionality - How does NARIMA® Color Effect Glass works?