AS 87 eco

Strong and durable, with excellent transmission and bending strength, AS 87 eco is the ideal cover and sensor glass material. The unique production process for this ultra-thin glass not only means it has a precise geometry, but also cuts out the need for a secondary glass slimming process.

Sharp view through a strong material

Low thickness, ultra-high strength

As the world’s first low thickness and ultra-high strength glass available in mass production, AS 87 eco offers a cost-effective option for consumer electronics. The ultra-thin glass improves the sensitivity of touchscreens while maintaining a strong protective role.

High impact and bending strength

The latest smartphones require highly durable glass covers, and the high impact and bending strength of AS 87 eco provides exceptional levels of protection for these sensitive devices. This impressive strength also enables the development of thinner, sleeker and more sensitive devices.

Exceptional geometric properties

The manufacture of AS 87 eco involves direct hot-forming of the glass, which results in extremely precise geometric properties such as a tight thickness tolerance of ± 20 µm or lower. With no requirement for a secondary glass slimming process, SCHOTT will direct ship AS 87 eco to the customer.

Excellent transmission characteristics

With a transmission of 92 %, AS 87 eco is ideal for cover glass and sensor protection for smartphones, which both require extremely high levels of transmission. As smartphone displays become sharper and sensors become more sensitive, their cover glasses need to keep pace.

Thermal properties

Chart showing the thermal properties of AS 87 eco glass

Electrical properties

Chart showing the electrical properties of AS 87 eco glass

Chemical properties

Chart showing the chemical properties of AS 87 eco glass

Mechanical properties

Chart showing the mechanical properties of AS 87 eco glass

Optical properties

Chart showing the optical properties of AS 87 eco glass

 

Chart showing the spectral transmittance of AS 87 eco glass (200-3200 nm)

 

Chart showing the spectral transmittance of AS 87 eco glass (200-450 nm)

 

Chart showing the transmittance values of AS 87 eco glass

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Get in touch
Man in glasses in business office on phone while working on laptop_605x350.jpg