Product Variants of Glass Tubing with High UV Transmission
SCHOTT 8337B
CHARACTERISTICS
This makes it especially suitable for the manufacture of UV lamps and detectors, as well as photomultipliers.
YOUR ADVANTAGES
- Offers the possibility for direct sealing to the alloy Kovar or tungsten.
 
SCHOTT 8347
CHARACTERISTICS
Due to its high hydrolytic resistance it can be used for water disinfection purposes as well as light guides.
YOUR ADVANTAGES
- High UVC transmission.
 - Higher IR transmittance (Infrared) than standard borosilicate glass tubing 3.3.
 
SCHOTT RayVolution® D 99
CHARACTERISTICS
This makes it especially suitable as envelope for germicidal lamps (low-pressure mercury vapour discharge lamps).
YOUR ADVANTAGES
- Outstanding high UV-C transmissivity.
 - High geometrical and cosmetic quality.
 
RayVolution® L 41 for UV LED
CHARACTERISTICS
Besides its excellent UVC transmission values, its thermal expansion is very close to aluminium nitride.
YOUR ADVANTAGES
- Glass wafer for LED optics.
 - Facilitates the optics manufacturing for LED Package on wafer level.
 
Discs for UV sensors
CHARACTERISTICS
These discs offer outstanding UV transmission and low solarization.
YOUR ADVANTAGES
- Form is ready for installation without further processing.
 - Direct sealing options with common electrode materials.