Titanium hermetic packaging

Glass-to-titanium sealing technology brings together advanced hermetic packaging and the exceptional properties of titanium. On this page, you’ll discover why titanium is a game-changer for industries like medical, aerospace, and oil & gas. Dive into its benefits, technical details, and SCHOTT’s innovative products and expertise.
Introduction

What is glass-to-titanium sealing?

Glass-to-titanium sealed hermetic components are created using a specialized glass-to-metal sealing technique. In this process, titanium functions as the housing material while specialty glass provides electrical insulation and enhances RF functionality. This produces durable, hermetically glass-sealed titanium packages, headers, and feedthroughs that reliably protect electronics while delivering all the advantages of titanium.
Titanium housing with hermetic components and connectors

Titanium packages

Robust, lightweight and non-magnetic titanium housings can protect multi-chip modules and optoelectronic circuit boards from harsh environmental conditions.

Titanium connectors

Lightweight, autoclavable titanium connectors with multiple feedthroughs and alignment structures are suitable for endoscopy and sensor applications.

Titanium-framed windows

Optical windows integrated into titanium housings provide options for signal, image, and energy transfer into active implants and sensor housings.

Titanium battery seals

Titanium battery seals provide a chemically stable and biocompatible option for implantable batteries.

Titanium weld inserts

Small weld inserts with multiple feedthroughs can be integrated into larger titanium housings using laser beam welding.

Titanium packages

Titanium connectors

Titanium-framed windows

Titanium battery seals

Titanium weld inserts

Benefits
Applications

Applications

Titanium’s unique combination of properties makes it an ideal material for packaging, encapsulating, and connecting electronic components, especially in challenging environments.

    Offshore wind turbines in the ocean for renewable energy
    1/5

    Energy and renewables

    Titanium protects sensors and connectors in energy systems, such as offshore wind turbines, solar monitoring devices, and hydrogen fuel systems, from corrosive environments.
    GettyImages-1416029563.jpg
    2/5

    Wearables

    Titanium’s lightweight, durable, and corrosion-resistant nature makes it ideal for wearable devices such as smartwatches, fitness trackers, and AR glasses. It protects electronics from moisture while also enhancing product longevity.
    X-ray image showing pacemaker with titanium housing
    3/5

    Medical electronics

    Titanium is the established standard for sealing electronics in medical implants like pacemakers and neurostimulators. With proven biocompatibility and biostability, life-saving electronics can be protected against bodily fluids and provide reliable performance for years.
    Learn more
    Rocket launch pad with spacecraft prepared for takeoff
    4/5

    Aerospace & defense

    In aerospace and defense, titanium is indispensable for protecting avionics and control systems. Lightweight yet strong, it encapsulates sensitive electronics, enabling devices to withstand extreme temperatures, pressure, and vibrations. Titanium’s non-magnetic and corrosion-resistant properties make it ideal for connectors and housings in mission-critical defense equipment.
    Learn more
    Offshore oil platform illuminated at sunset in open sea
    5/5

    Oil & gas / marine electronics

    Titanium’s resistance to saltwater, high pressure, and corrosive chemicals makes it ideal for subsea exploration, drilling, and production equipment. It is also used in sensors and communication systems in geophysical exploration, marine navigation, and desalination systems.
    Technology

    Technical details

    SCHOTT leverages decades of experience in glass development, laser welding, active brazing, and material bonding to deliver tailored solutions. From mastering the fundamentals of glass-to-titanium sealing to supporting new processing techniques, SCHOTT combines precision engineering and in-house capabilities to enable robust, high-performance hermetic components.

    The following Q&A explores key technologies and processes that enable SCHOTT to meet titanium hermetic packaging requirements.

    Glass-to-titanium sealing is a highly specialized technology that draws on advanced specialty glass know-how and glass-to-metal sealing expertise. Specially formulated glass enables the reliable joining of titanium and glass, materials that are typically difficult to combine. Careful surface preparation is required for reliable adhesion, despite titanium's natural tendency to form surface oxide layers.

    With precise heat management, controlled assembly processes, and thorough post-sealing control, we can manufacture robust, hermetic seals that meet the highest standards of reliability and durability. SCHOTT’s advanced expertise allows us to deliver these complex components for demanding applications.

    SCHOTT’s modular approach and in-house capabilities provide customers with tailored solutions for even the most complex titanium hermetic packaging requirements. From active brazing, laser welding, and titanium-nickel bonding to using MIM parts for cost-efficient manufacturing, we combine materials knowledge and precision engineering to deliver reliable, high-performance products for demanding industries.

    Comprehensive solutions for titanium hermetic packaging

    Beyond our extensive glass expertise, SCHOTT offers a wide range of modular solutions to address the challenges of titanium hermetic packaging and create additional value for our customers. These solutions enable us to handle complex designs, integrate multiple functionalities, and offer long-term reliability in demanding applications.

    Titanium hermetic packages often require intricate designs to meet specific application needs. Our experience in combining materials and advanced manufacturing techniques allows us to handle even the most complex requirements:

    • Electrical feedthroughs: Our glass-to-titanium sealing technology provides reliable hermeticity and electrical insulation for feedthroughs.
    • Optical windows: Integrating optical windows into titanium housings requires advanced processes such as active brazing and laser welding.
    • Thermal management: Materials used in hermetic housings often exhibit vastly different thermal expansion coefficients. SCHOTT has developed reliable processes for integrating common heat sink materials such as molybdenum into titanium housings for optimized heat management.
    • Surface modification: Surfaces can be post-treated to generate solderable or wire-bondable conditions. Also, selective process options are available.

    As a glass inventor, SCHOTT’s ongoing in-house glass development is the “secret sauce” for advancing titanium hermetic packaging. We create and refine glasses that are specifically designed to bond directly with titanium. Our ability to control the entire development process—from material innovation to final production—offers superior quality and performance and allows us to develop entirely new glass formulations tailored to meet unique customer or application-specific requirements. This gives SCHOTT a distinct advantage in delivering cutting-edge solutions for demanding applications.

    1. Advanced autoclavable glass for titanium packages in medical applications
      Traditionally, CaBaL12 glass was used with titanium medical devices due to its established compatibility. However, this glass has limited hydrolytic resistance after extended use, particularly under repeated autoclave cycles. To address this challenge, SCHOTT developed advanced autoclavable glasses that bond directly with titanium, providing durability, enhanced hydrolytic resistance, and reliable long-term performance.

    2. Implantable glass for titanium packaging with proven biocompatibility
      With titanium-sealing glasses for implantable devices, the number of components for hermetic seals can be reduced, allowing smaller footprints and highly customized designs. 

    3. High-performance sealing glass for hermetic titanium components in high-pressure, high-temperature (HPHT) applications
      SCHOTT sealing glasses, designed for extreme (HPHT) environments, directly bond with titanium to create robust hermetic seals. These glasses are engineered to withstand high temperatures and intense vibrations, meeting the stringent demands of oil and gas applications, for example. The combination of titanium packaging and SCHOTT’s specialized glass know-how offer exceptional and consistent component quality.

    SCHOTT’s in-house laser welding expertise enables the design and manufacture of precise hermetic seals with minimal heat-affected zones, preserving material properties and meeting tight tolerances. For titanium packages, we can process small components and integrate them into larger titanium housings. Examples include:

    • Connectors and ports: These components can be individually processed, plated, and hermetically welded into the housing to create complex, multi-functional packages.
    • Solderable coatings: Solderable surfaces can be integrated where needed, enabling easy assembly of other components in customer systems.
    • Corrosion-resistant weld seams: Welded areas regain a passive surface after welding, providing long-term corrosion protection.

    Active brazing is a core capability at SCHOTT, enabling us to deliver high-performance, hermetic solutions for demanding applications in industries such as medical, aerospace, and energy. Here are two examples:

    • Sapphire-to-titanium bonding: Sapphire, a preferred material for optical windows, cannot be bonded using standard solders without proper metallization. SCHOTT uses a specialized active brazing process with a titanium-containing braze to directly bond sapphire discs to titanium frames without the need for additional metallization.
    • Molybdenum and titanium integration: Active brazing enables robust connections for molybdenum and titanium, supporting complex thermal management solutions and high mechanical stability.

    Many customers don’t realize that metal injection molded components can be hermetic, assuming some porosity is always present. SCHOTT has demonstrated that MIM can deliver both hermeticity and cost efficiency:

    • Hermeticity: MIM components can be designed and manufactured to meet strict hermeticity standards, making them suitable for critical applications.
    • Cost efficiency: Especially for higher production volumes, MIM parts are significantly more cost-effective than traditionally milled titanium housings, making them ideal for large-scale applications.
    Products and expertise

    Products


    Explore SCHOTT’s custom-designed products featuring glass-to-titanium sealing technology. The image gallery showcases examples designed for demanding applications across industries. To dive deeper, visit the links to related product pages where this innovative technology can be applied.

    Worker checking glass to metal

    Why choose SCHOTT as your supplier?

    By combining your needs with our expertise and innovation, we deliver exceptional customer value. Explore case studies and testimonials showcasing the joint creation of hermetic components. Together, we ensure top performance, durability, and cost-efficiency for your projects.

    Learn more

    Want to know more? Let’s talk.

    Whether you need more information or advice for a project, I would be delighted to talk to you.

    Dr. Eveline Rudigier-Voigt

    Dr. Eveline Rudigier-Voigt

    Head of Development and Technology Center

    *Required field

    SCHOTT will only use your data to respond to your inquiry. For more information, please click here.