Product variants of customized enclosures and feedthroughs for implantable medical devices
Feedthroughs for implantable devices
CHARACTERISTICS
- Electrolyte-resistant glass sealing: Can provide long-lasting protection against harsh chemical environments in implantable batteries.
- Customized design: Options to precisely tailor the number of pins and ground pin configurations. Weldable or solderable surfaces are also available.
- Proven material combinations: Established materials with a track record of success in critical medical applications.
- Decades of expertise: Built on decades of innovation in glass-to-metal sealing technologies.
YOUR ADVANTAGES
- Exceptional reliability: Can contribute to consistent performance and patient safety over the device’s lifetime.
- Tailored solutions: Fully adaptable to meet unique technical and design requirements.
- Enhanced device trustworthiness: Backed by a history of proven success.
- Future-ready durability: Precision engineering combined with robust materials for long-term dependability.
Battery Lids for implantable devices
CHARACTERISTICS
- Ultra-compact design:
Thickness: Less than 0.5 mm.
Diameter: Less than 2 mm. - Secure glass sealing: Electrolyte-resistant glass ensures reliable encapsulation of lithium-ion battery chemistry.
- Biocompatible materials: Lid and pins made from materials safe for use in the body, e.g. Titanium and Platinum/Platinum-Iridium.
- Customizable engineering: Fully tailored designs to meet unique device requirements, such as neurostimulators, cochlear implants, and cardiac devices.
YOUR ADVANTAGES
- Enables miniaturization: Ultra-thin, compact design supports the development of smaller, less invasive devices.
- Long-term safety: A reliable seal protects the battery chemistry and can contribute to the safety and longevity of the device.
- Biocompatibility: Materials certified safe for patient use minimize health risks.
- Custom solutions for broad applications: Tailored designs provide seamless integration with specific medical applications, such as neurostimulators, cochlear implants, and cardiac devices.