Xensation®

The SCHOTT Xensation® family of products comprises a broad range of state-of-the-art glass covers for a fast-moving electronics market. The portfolio offers outstanding aesthetic, optical and haptical properties, as well as unrivalled durability, flexibility and strength.

Tough, flexible and strong, with high transmission

Improved chemical strengthening

The Xensation® family benefits from a salt bath process that increases ion exchange (IOX). The process displaces small ions, allowing larger ions to move in, which means the space is better filled and the material is more stable.

High transparency

The high-resolution displays of smartphones and other electronic devices demand exceptional cover glasses. With excellent transparency and high transmission, Xensation® is the ideal match for displays, delivering high optical quality for the clearest view.

Flexibility like never before

SCHOTT’s unrivalled reputation for innovation and expertise is proven by the introduction of Xensation® Flex, an ultra-thin glass designed for foldable glass covers that offers a very low bending radius of less than 2 mm.

Made to survive

SCHOTT Xensation® α a lithium alumino-borosilicate (LABS) glass unites the chemical strengthening potential of LAS glass with the scratch performance of borosilicate glass and a strong glass backbone like in glass-ceramics. A true high performance cover glass which outperforms current market leading cover glasses by up to 100% in set-drop performance on all grounds, including rough surfaces.

Xensation® α

SCHOTT’s worldwide unequalled innovation power has paved the way for those successful new glass developments and created the latest invention: Xensation® α – a lithium alumino-borosilicate (LABS) glass.

  • Outstanding break resistance – 100% better set drop performance compared to leading cover glasses.
  • Significantly improved scratch resistance – shown in Knoop indenter scratch test.
  • Perfect optical transparency.
  • Optimized IOX exchange for an even tougher surface.

Xensation® α placed on a smartphone dummy in a set drop testing device.
Xensation® α delivers one of the highest drop performances in the market.

 

Xensation® Flex

SCHOTT Xensation® Flex offers the ability to produce high quality foldable devices with an extraordinary bending radius. Other advantages include:

  • Specially developed for chemical toughening.
  • High flexibility and small bending radius.
  • Excellent transparency and transmission.
  • Fire-polished premium surface.

 

Material testing equipment conducting a three-point bending test on a sample of glass

3 point bending test.

Xensation® Up.

The high-strength SCHOTT Xensation® Up. glass produces outstanding results in set drop tests, ensuring maximum survival likelihood after smartphone drops. Other key properties include:

  • Superior ion exchange capabilities for excellent strength and processing performance.
  • Increased flexibility for maximum strength performance.
  • Wider IOX processing ranges.
  • Options for shorter IOX processing time.
  • Typical CS (compressive stress) and DoL (depth of layer) values are evenly balanced to obtain superior mechanical reliability.

 

Laboratory machine performing a drop test on a smartphone fitted with Xensation® Up.

SCHOTT Xensation® Up. can withstand a drop of almost double the height of conventional cover glass.

 

Xensation® 3D

Xensation® 3D fulfills a range of technical requirements for cover glass, including:

  • Extra-high fracture toughness.
  • High resistance against impacts and scratches.
  • High scratch tolerance – low breakage risk even with surface scratches.
  • Chemical strengthening parameters able to be adjusted to achieve desired level of strength for specific applications.
  • High chemical durability.
  • High light transmission.
 

Laboratory machine performing a bending test on a sample of ultra-thin glass

SCHOTT Xensation® 3D is extremely robust with high light transmission.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Spojte se s námi
Man in glasses in business office on phone while working on laptop_605x350.jpg