Cut-to-Size Substrates

SCHOTT is committed to innovation and excellence, which is why our products’ technical properties set a uniform high standard. From CTE range to production techniques, our extensive portfolio of cut-to-size substrate glasses offer a proven ability to perform in all situations to the highest of standards.

Technical excellence across the board

Broad CTE range

SCHOTT cut-to-size substrates are designed to perform in a wide range of environments, which is why their coefficient of thermal expansion (CTE) is a key consideration. With CTEs ranging from 3.2 x 10⁻⁶ / ºC – 9.4 x 10⁻⁶ / ºC, there are few fields in which SCHOTT glass cannot meet the challenge.

Thicknesses and sizes to suit

SCHOTT glass cut-to-size substrates have to perform reliably and fit precisely in a variety of applications. We achieve this by offering multiple cut-to-size formats and thicknesses ranging from 0.03 mm up to 25.40 mm.

Mastery of production techniques

SCHOTT employs a number of unique hot forming methods, including down-draw for thin glass, up-draw for homogeneous clear flat glasses, and microfloat for robust chemical and thermal properties. In addition, our cutting, seaming, and laser-marking methods set new industry standards.

Quality processing

All SCHOTT processing methods strictly follow the latest international industry standards, with a number of customization options available. Whatever method suits your requirements, we are always happy to work with you to create a tailored solution.

Up-drawn cut-to-size substrates

The following specifications are applicable to B 270® i: 

 

Cutting formats

Chart showing the cutting formats of up-drawn B 270® i cut-to-size substrates

 

Glass quality properties

Chart showing the glass quality properties of up-drawn B 270® i cut-to-size substrates

Down-drawn cut-to-size substrates

The following specifications are applicable to D 263® T eco, D 263® LA eco, AF 32® eco, Solar Glass 0787and B 270® D:

 

Base material  formats

Chart showing the base material formats of down-drawn cut-to-size substrates

 

Geometrical properties

Chart showing the geometrical properties of base material cut-to-size substrates

 

Cutting formats

Chart showing the cutting formats of down-drawn cut-to-size substrates

 

Glass quality properties

Chart showing the glass quality properties of down-drawn cut-to-size substrates

 

Floated cut-to-size substrates

The following specifications are applicable to BOROFLOAT®:

 

Chart showing the cutting formats of BOROFLOAT®

Cut-to-size substrate materials

The following materials are available as cut-to-size substrates:

  • D 263® T eco
  • D 263® LA eco
  • BOROFLOAT®
  • AF 32® eco
  • B 270® 
  • Solar Glass 0787

 To find out more, please see the related materials on the overview page.

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Spojte se s námi
Man in glasses in business office on phone while working on laptop_605x350.jpg