PYRAN® Platinum is available as three different products: the monolithic glass-ceramic PYRAN® Platinum, the laminated PYRAN® Platinum L, and PYRAN® Platinum F, which features a surface-applied film. PYRAN® Platinum L and F offer high impact resistance alongside protection from fire, hot gases and smoke.
PYRAN® Platinum
PYRAN® Platinum

PYRAN® Platinum fire-rated glazing material is made from the world’s first and only floated transparent glass-ceramic. It is intended for use in non-impact, non-safety-rated locations such as transoms and windows with fire-rating requirements up to 90 minutes.

CHARACTERISTICS

With a thickness of 3/16" (5 mm), PYRAN® Platinum provides fire protection for up to 90 minutes with the required hose-stream test. Clear and colorless, the glass-ceramic also offers a smooth surface and distortion-free mirror finish, making it ideal for architectural applications.


YOUR ADVANTAGES

  • Available in sheet size 51 x 99” – the largest in the industry.
  • Weight: 2.6 lbs/ft²
  • Can be used to construct insulated glazing units.
  • Able to be lightly sandblasted or delivered with surface-applied opacity film without affecting the fire-rating.
  • Produced without the hazardous heavy metals antimony and arsenic.
PYRAN® Platinum L
PYRAN® Platinum L

Thanks to an added lamination process, this impact- and fire-rated glass-ceramic is designed to be used in doors and windows with a high risk of accidents. PYRAN® Platinum L not only remains intact after heavy impact, but features the same high resistance to heat and thermal shock as PYRAN® Platinum.

CHARACTERISTICS

With a thickness of 3/8” (9 mm), PYRAN® Platinum L provides fire protection for up to 90 minutes in windows and up to three hours in doors, both with the required hose stream test. Clear and colorless, the glass-ceramic also offers a smooth surface and distortion-free mirror finish, making it ideal for architectural applications.


YOUR ADVANTAGES

  • Available in sheet size 51 x 99” – the largest in the industry.
  • Transparent and wireless.
  • Weight: 4.3 lbs/ft².
  • Achieves the positive pressure test standard UL 10C.
  • Can be used to construct insulated glazing units.
  • Can be lightly sandblasted or delivered with surface-applied opacity film, without affecting the fire-rating.
  • Produced without the hazardous heavy metals antimony and arsenic.
  • Impact rating: ANSI Z97.1 (Class A) and CPSC 16CFR1201 (Cat. I and II).
PYRAN® Platinum F
PYRAN® Platinum F

Ideal for safety-rated locations such as windows, door lites, transoms and sidelites, PYRAN® Platinum F features a surface-applied safety film that adds impact resistance to outstanding heat resistance. With the same thickness, sheet size, fire rating and stunning appearance as PYRAN® Platinum, this variant adds an extra layer of safety to your doors and windows.

CHARACTERISTICS

Designed to withstand impact as well as heat, hose stream and thermal shock, this clear, colorless glass-ceramic is fire-rated for up to 90 minutes in windows and up to 180 minutes in doors. Achieving the positive pressure test standard UL 10C, PYRAN® Platinum F can also be lightly sandblasted or delivered with surface-applied opacity film, without affecting its fire rating.


YOUR ADVANTAGES

  • Available in sheet size 51 x 99” – the largest in the industry – and a thickness of 3/16” (5 mm).
  • Weight: 2.6 lbs/ft².
  • Microfloat production process results in a smooth surface and distortion-free mirror finish with surface-applied safety film.
  • Clear and colorless without a distracting amber tint.
  • Can be used to construct insulated glazing units.
  • Produced without the hazardous heavy metals antimony and arsenic.
  • Impact rating: ANSI Z97.1 and CPSC 16CFR1201 (Cat. I and II).

Want to know more? Let's talk

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

Get in touch
Daniel Poling, Business Development & Sales Manager
Daniel Poling

Business Development & Sales Manager