Technical Details of Battery Lids and Connectors
Specifications
Lithium Primary Battery Covers | Lithium-Ion Battery Covers | SCHOTT Minicaps™ | Ultracapacitor/ Aluminum Electrolyte Capacitor Covers | Battery connector | |
---|---|---|---|---|---|
Gas-tightness | 1 x 10-8mbar x l/s | 1 x 10-8mbar x l/s |
1 x 10-8mbar x l/s | 1 x 10-8mbar x l/s | 1 x 10-8mbar x l/s |
Electrical Isolation | 108Ω to 109Ω |
Small designs:108Ω to 109Ω Large designs:107Ω to 108Ω |
1010Ω |
Small designs:108Ω to 109Ω Large designs:107Ω to 108Ω |
108Ω to 109Ω |
Chemical resistance | High, against wide range of standard electrolytes incl. LiSO2, LiSOCL2, LiMnO2 | High, against range of standard electrolytes |
High, against range of standard electrolytes | High, against range of standard electrolytes | High, against range of standard electrolytes |
Temperature stability | High: from -65 °C to + 150 °C |
High: from -65 °C to + 150 °C |
High: from -40 °C to + 150 °C |
High: from -40 °C to + 150 °C |
High: from -65 °C to + 150 °C |
Pressure tightness | Very high | High to very high, depending on dimension | 10 N to 100 N and more, depending on design | High to very high, depending on dimension | Very high |
Mechanical strength | Very high | High to very high, depending on dimension | 10 N to 100 N and more, depending on design | High to very high, depending on dimension | Very high |
Sealing material | Glass | Glass | Glass | Glass | Glass |
Pins | Steel, Nickel Iron Alloys | Aluminum, Copper, Steel, Nickel Iron Alloys | Stainless Steel/ Nickel Alloy | Aluminum | Stainless Steel/ Nickel Alloy |
Lid | Steel, Stainless Steel | Aluminum, Stainless Steel | Stainless Steel | Aluminum, Copper | Steel, Stainless Steel |
Lifetime | Up to 25 years | Up to 25 years | Up to 25 years |
Up to 25 years | Up to 25 years |
Lithium Primary Battery Covers | Lithium-Ion Battery Covers | SCHOTT Minicaps™ | Ultracapacitor/ Aluminum Electrolyte Capacitor Covers | Battery connector | |
---|---|---|---|---|---|
Gas-tightness | 1 x 10-8mbar x l/s | 1 x 10-8mbar x l/s |
1 x 10-8mbar x l/s | 1 x 10-8mbar x l/s | 1 x 10-8mbar x l/s |
Electrical Isolation | 108Ω to 109Ω |
Small designs:108Ω to 109Ω Large designs:107Ω to 108Ω |
1010Ω |
Small designs:108Ω to 109Ω Large designs:107Ω to 108Ω |
108Ω to 109Ω |
Chemical resistance | High, against wide range of standard electrolytes incl. LiSO2, LiSOCL2, LiMnO2 | High, against range of standard electrolytes |
High, against range of standard electrolytes | High, against range of standard electrolytes | High, against range of standard electrolytes |
Temperature stability | High: from -65 °C to + 150 °C |
High: from -65 °C to + 150 °C |
High: from -40 °C to + 150 °C |
High: from -40 °C to + 150 °C |
High: from -65 °C to + 150 °C |
Pressure tightness | Very high | High to very high, depending on dimension | 10 N to 100 N and more, depending on design | High to very high, depending on dimension | Very high |
Mechanical strength | Very high | High to very high, depending on dimension | 10 N to 100 N and more, depending on design | High to very high, depending on dimension | Very high |
Sealing material | Glass | Glass | Glass | Glass | Glass |
Pins | Steel, Nickel Iron Alloys | Aluminum, Copper, Steel, Nickel Iron Alloys | Stainless Steel/ Nickel Alloy | Aluminum | Stainless Steel/ Nickel Alloy |
Lid | Steel, Stainless Steel | Aluminum, Stainless Steel | Stainless Steel | Aluminum, Copper | Steel, Stainless Steel |
Lifetime | Up to 25 years | Up to 25 years | Up to 25 years |
Up to 25 years | Up to 25 years |