Lead-free Transistor Outline Caps
About
The transistor outline caps fulfill two primary functions. First, they protect the optical components of transmission as well as reception applications. Second, they ensure the transmission of the optical signals by acting as an optical interface.
Product features
- Special granulation method developed for versatility in design of Pb-free solder glass
 - No compromise of adhesion and chemical stability
 - Existing caps can be switched to fully RoHS compliant version
 - Ready for expiry and non-extension of EU RoHS exemptions 7c-I