RG680

RG680
承诺光谱值
λsi = 0.00001) [nm] 595
λci = 0.5) [nm] 680 ± 6
您需要帮助或报价吗?
与我们的支持团队联系
技术规格
内部透过率(图表)

仅允许1到30之间的值,小数点保留一位。

SCHOTT
RG680 - RG680
厚度
3.0
反射系数
0.9135
内部透过率(表格)
λ [nm]
200 < 10⁻³
210 < 10⁻³
220 < 10⁻³
230 < 10⁻³
240 < 10⁻³
250 < 10⁻³
260 < 10⁻³
270 < 10⁻³
280 < 10⁻³
290 < 10⁻³
300 < 10⁻³
310 < 10⁻³
320 < 10⁻³
330 < 10⁻³
340 < 10⁻³
350 < 10⁻³
360 < 10⁻³
370 < 10⁻³
380 < 10⁻³
390 < 10⁻³
400 < 10⁻³
410 < 10⁻³
420 < 10⁻³
430 < 10⁻³
440 < 10⁻³
450 < 10⁻³
460 < 10⁻³
470 < 10⁻³
480 < 10⁻³
490 < 10⁻³
λ [nm]
500 < 10⁻³
510 < 10⁻³
520 < 10⁻³
530 < 10⁻³
540 < 10⁻³
550 < 10⁻³
560 < 10⁻³
570 < 10⁻³
580 < 10⁻³
590 < 10⁻³
600 < 10⁻³
610 < 10⁻³
620 < 10⁻³
630 < 10⁻³
640 < 10⁻³
650 0.001
660 0.024
670 0.180
680 0.510
690 0.774
700 0.899
710 0.948
720 0.967
730 0.974
740 0.977
750 0.978
760 0.978
770 0.978
780 0.977
790 0.976
λ [nm]
800 0.976
810 0.975
820 0.975
830 0.974
840 0.974
850 0.974
860 0.973
870 0.973
880 0.973
890 0.973
900 0.973
910 0.973
920 0.973
930 0.973
940 0.973
950 0.973
960 0.973
970 0.973
980 0.973
990 0.973
1,000 0.973
1,010 0.973
1,020 0.973
1,030 0.973
1,040 0.973
1,050 0.973
1,060 0.973
1,070 0.973
1,080 0.974
1,090 0.973
λ [nm]
1,100 0.974
1,110 0.974
1,120 0.974
1,130 0.974
1,140 0.974
1,150 0.975
1,160 0.975
1,170 0.975
1,180 0.976
1,190 0.976
1,200 0.976
1,250 0.978
1,300 0.979
1,350 0.981
1,400 0.983
1,450 0.985
1,500 0.988
1,550 0.989
1,600 0.990
1,650 0.990
1,700 0.989
1,750 0.988
1,800 0.987
1,850 0.985
1,900 0.985
1,950 0.985
2,000 0.984
2,050 0.983
2,100 0.982
2,150 0.979
λ [nm]
2,200 0.970
2,250 0.967
2,300 0.969
2,350 0.970
2,400 0.968
2,450 0.966
2,500 0.964
2,550 0.963
2,600 0.962
2,650 0.957
2,700 0.921
2,750 0.606
2,800 0.426
2,850 0.401
2,900 0.400
2,950 0.397
3,000 0.386
3,050 0.367
3,100 0.346
3,150 0.324
3,200 0.302
3,250 0.282
3,300 0.267
3,350 0.256
3,400 0.253
3,450 0.258
3,500 0.268
3,550 0.282
3,600 0.297
3,650 0.312
λ [nm]
3,700 0.326
3,750 0.338
3,800 0.348
3,850 0.356
3,900 0.363
3,950 0.366
4,000 0.363
4,050 0.352
4,100 0.331
4,150 0.305
4,200 0.277
4,250 0.239
4,300 0.191
4,350 0.142
4,400 0.092
4,450 0.050
4,500 0.023
4,550 0.010
4,600 0.004
4,650 0.002
4,700 < 10⁻³
4,750 < 10⁻³
4,800 < 10⁻³
4,850 < 10⁻³
4,900 < 10⁻³
4,950 < 10⁻³
5,000 < 10⁻³
5,050 < 10⁻³
5,100 < 10⁻³
5,150 < 10⁻³
光学值
反射系数
Pd 0.914
参考厚度
d [mm] 3
承诺光谱值
λsi = 0.00001) [nm] 595
λci = 0.5) [nm] 680 ± 6
折射率 n
ns (852.1 nm) = 1.530
nd (587.6 nm) = 1.540
色度评估
光源 A(Planck T = 2347K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
光源 Planck T = 3200 K
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
光源 D65 (TC = 6504 K)
d [mm] 1 2 3
x
y
Y
λd [nm]
Pe
物理值
密度
p [g/cm3] 2.76
气泡含量
气泡等级 3
玻转温度
Tg [°C] 532
温度系数
Tk [nm/°C] 0.18
耐化学性
耐污性 0
耐酸性 1.0
耐碱性 1.0
热膨胀
α-30°C/+70°C [10-6/K] 8.1
α20°C/300°C [10-6/K] 9.4
α20°C/200°C [10-6/K]