技术规格
内部透过率(图表)
- SCHOTT
- BG66HS - BG66HS
- 厚度
- 1.0
- 反射系数
- 0.9130
内部透过率(表格)
| λ [nm] | |
|---|---|
| 200 | |
| 210 | |
| 220 | |
| 230 | |
| 240 | |
| 250 | |
| 260 | |
| 270 | |
| 280 | |
| 290 | |
| 300 | |
| 310 | |
| 320 | < 10⁻³ |
| 330 | < 10⁻³ |
| 340 | 0.037 |
| 350 | 0.185 |
| 360 | 0.375 |
| 370 | 0.526 |
| 380 | 0.623 |
| 390 | 0.685 |
| 400 | 0.728 |
| 410 | 0.760 |
| 420 | 0.786 |
| 430 | 0.809 |
| 440 | 0.829 |
| 450 | 0.847 |
| 460 | 0.863 |
| 470 | 0.876 |
| 480 | 0.886 |
| 490 | 0.893 |
| λ [nm] | |
|---|---|
| 500 | 0.895 |
| 510 | 0.890 |
| 520 | 0.875 |
| 530 | 0.848 |
| 540 | 0.804 |
| 550 | 0.741 |
| 560 | 0.660 |
| 570 | 0.564 |
| 580 | 0.460 |
| 590 | 0.356 |
| 600 | 0.260 |
| 610 | 0.179 |
| 620 | 0.115 |
| 630 | 0.071 |
| 640 | 0.041 |
| 650 | 0.022 |
| 660 | 0.011 |
| 670 | 0.006 |
| 680 | 0.003 |
| 690 | 0.001 |
| 700 | < 10⁻³ |
| 710 | < 10⁻³ |
| 720 | < 10⁻³ |
| 730 | < 10⁻³ |
| 740 | < 10⁻³ |
| 750 | < 10⁻³ |
| 760 | < 10⁻³ |
| 770 | < 10⁻³ |
| 780 | < 10⁻³ |
| 790 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 800 | < 10⁻³ |
| 810 | < 10⁻³ |
| 820 | < 10⁻³ |
| 830 | < 10⁻³ |
| 840 | < 10⁻³ |
| 850 | < 10⁻³ |
| 860 | < 10⁻³ |
| 870 | < 10⁻³ |
| 880 | < 10⁻³ |
| 890 | < 10⁻³ |
| 900 | < 10⁻³ |
| 910 | < 10⁻³ |
| 920 | < 10⁻³ |
| 930 | < 10⁻³ |
| 940 | < 10⁻³ |
| 950 | < 10⁻³ |
| 960 | < 10⁻³ |
| 970 | < 10⁻³ |
| 980 | < 10⁻³ |
| 990 | < 10⁻³ |
| 1,000 | < 10⁻³ |
| 1,010 | < 10⁻³ |
| 1,020 | < 10⁻³ |
| 1,030 | < 10⁻³ |
| 1,040 | < 10⁻³ |
| 1,050 | < 10⁻³ |
| 1,060 | < 10⁻³ |
| 1,070 | < 10⁻³ |
| 1,080 | < 10⁻³ |
| 1,090 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 1,100 | < 10⁻³ |
| 1,110 | < 10⁻³ |
| 1,120 | < 10⁻³ |
| 1,130 | < 10⁻³ |
| 1,140 | < 10⁻³ |
| 1,150 | < 10⁻³ |
| 1,160 | 0.001 |
| 1,170 | 0.001 |
| 1,180 | 0.002 |
| 1,190 | 0.002 |
| 1,200 | 0.003 |
| 1,250 | 0.006 |
| 1,300 | 0.015 |
| 1,350 | 0.031 |
| 1,400 | 0.058 |
| 1,450 | 0.097 |
| 1,500 | 0.154 |
| 1,550 | 0.216 |
| 1,600 | 0.282 |
| 1,650 | 0.350 |
| 1,700 | 0.421 |
| 1,750 | 0.488 |
| 1,800 | 0.551 |
| 1,850 | 0.606 |
| 1,900 | 0.655 |
| 1,950 | 0.699 |
| 2,000 | 0.735 |
| 2,050 | 0.766 |
| 2,100 | 0.793 |
| 2,150 | 0.815 |
| λ [nm] | |
|---|---|
| 2,200 | 0.832 |
| 2,250 | 0.847 |
| 2,300 | 0.858 |
| 2,350 | 0.871 |
| 2,400 | 0.880 |
| 2,450 | 0.886 |
| 2,500 | 0.889 |
| 2,550 | 0.894 |
| 2,600 | 0.894 |
| 2,650 | 0.893 |
| 2,700 | 0.888 |
| 2,750 | 0.871 |
| 2,800 | 0.800 |
| 2,850 | 0.677 |
| 2,900 | 0.574 |
| 2,950 | 0.502 |
| 3,000 | 0.449 |
| 3,050 | 0.404 |
| 3,100 | 0.364 |
| 3,150 | 0.328 |
| 3,200 | 0.297 |
| 3,250 | 0.271 |
| 3,300 | 0.251 |
| 3,350 | 0.236 |
| 3,400 | 0.226 |
| 3,450 | 0.220 |
| 3,500 | 0.219 |
| 3,550 | 0.223 |
| 3,600 | 0.233 |
| 3,650 | 0.247 |
| λ [nm] | |
|---|---|
| 3,700 | 0.267 |
| 3,750 | 0.287 |
| 3,800 | 0.298 |
| 3,850 | 0.290 |
| 3,900 | 0.262 |
| 3,950 | 0.222 |
| 4,000 | 0.171 |
| 4,050 | 0.114 |
| 4,100 | 0.064 |
| 4,150 | 0.033 |
| 4,200 | 0.018 |
| 4,250 | 0.012 |
| 4,300 | 0.009 |
| 4,350 | 0.008 |
| 4,400 | 0.007 |
| 4,450 | 0.006 |
| 4,500 | 0.005 |
| 4,550 | 0.004 |
| 4,600 | 0.004 |
| 4,650 | 0.005 |
| 4,700 | 0.008 |
| 4,750 | 0.012 |
| 4,800 | 0.019 |
| 4,850 | 0.029 |
| 4,900 | 0.041 |
| 4,950 | 0.057 |
| 5,000 | 0.075 |
| 5,050 | 0.093 |
| 5,100 | 0.106 |
| 5,150 | 0.112 |
光学值
| 反射系数 | |
|---|---|
| Pd | 0.913 |
| 参考厚度 | |
|---|---|
| d [mm] | 1 |
| 承诺光谱值 | |
|---|---|
| τi (405nm) | ≥0.71 |
| τi (514nm) | ≥0.85 |
| τi (633nm) | ≥0.04 |
| τi (694nm) | ≤0.0025 |
| τi (1060nm) | ≤0.0004 |
| 折射率 n |
|---|
| nF (486.1 nm) = 1.548 |
| nh (404.7 nm) = 1.557 |
| ng (435.8 nm) = 1.553 |
| ns (852.1 nm) = 1.534 |
| ne (546.1 nm) = 1.544 |
| nd (587.6 nm) = 1.542 |
色度评估
| 光源 | A(Planck T = 2347K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.300 | 0.234 | 0.198 |
| y | 0.440 | 0.438 | 0.430 |
| Y | 47 | 32 | 23 |
| λd [nm] | 499 | 497 | 496 |
| Pe | 0.34 | 0.49 | 0.58 |
| 光源 | Planck T = 3200 K | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.283 | 0.222 | 0.190 |
| y | 0.419 | 0.413 | 0.403 |
| Y | 49 | 33 | 25 |
| λd [nm] | 497 | 496 | 495 |
| Pe | 0.35 | 0.50 | 0.59 |
| 光源 | D65 (TC = 6504 K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.217 | 0.182 | 0.164 |
| y | 0.313 | 0.298 | 0.288 |
| Y | 56 | 41 | 32 |
| λd [nm] | 489 | 489 | 488 |
| Pe | 0.36 | 0.50 | 0.58 |
物理值
| 密度 | |
|---|---|
| p [g/cm3] | 2.8705 |
| 气泡含量 | |
|---|---|
| 气泡等级 | |
| 玻转温度 | |
|---|---|
| Tg [°C] | 425 |
| 温度系数 | |
|---|---|
| Tk [nm/°C] | |
| 耐化学性 | |
|---|---|
| 耐污性 | |
| 耐酸性 | 52.3 |
| 耐碱性 | |
| 热膨胀 | |
|---|---|
| α-30°C/+70°C [10-6/K] | 11.47 |
| α20°C/300°C [10-6/K] | 13.33 |
| α20°C/200°C [10-6/K] | |