技术规格
内部透过率(图表)
- SCHOTT
- BG62HT - BG62HT
- 厚度
- 1.0
- 反射系数
- 0.9140
内部透过率(表格)
| λ [nm] | |
|---|---|
| 200 | |
| 210 | |
| 220 | |
| 230 | |
| 240 | |
| 250 | |
| 260 | |
| 270 | |
| 280 | |
| 290 | |
| 300 | |
| 310 | < 10⁻³ |
| 320 | < 10⁻³ |
| 330 | 0.006 |
| 340 | 0.095 |
| 350 | 0.304 |
| 360 | 0.509 |
| 370 | 0.642 |
| 380 | 0.721 |
| 390 | 0.769 |
| 400 | 0.802 |
| 410 | 0.826 |
| 420 | 0.846 |
| 430 | 0.863 |
| 440 | 0.878 |
| 450 | 0.892 |
| 460 | 0.904 |
| 470 | 0.912 |
| 480 | 0.919 |
| 490 | 0.925 |
| λ [nm] | |
|---|---|
| 500 | 0.926 |
| 510 | 0.921 |
| 520 | 0.909 |
| 530 | 0.886 |
| 540 | 0.848 |
| 550 | 0.794 |
| 560 | 0.723 |
| 570 | 0.636 |
| 580 | 0.537 |
| 590 | 0.434 |
| 600 | 0.334 |
| 610 | 0.243 |
| 620 | 0.168 |
| 630 | 0.111 |
| 640 | 0.069 |
| 650 | 0.041 |
| 660 | 0.023 |
| 670 | 0.013 |
| 680 | 0.007 |
| 690 | 0.003 |
| 700 | 0.002 |
| 710 | < 10⁻³ |
| 720 | < 10⁻³ |
| 730 | < 10⁻³ |
| 740 | < 10⁻³ |
| 750 | < 10⁻³ |
| 760 | < 10⁻³ |
| 770 | < 10⁻³ |
| 780 | < 10⁻³ |
| 790 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 800 | < 10⁻³ |
| 810 | < 10⁻³ |
| 820 | < 10⁻³ |
| 830 | < 10⁻³ |
| 840 | < 10⁻³ |
| 850 | < 10⁻³ |
| 860 | < 10⁻³ |
| 870 | < 10⁻³ |
| 880 | < 10⁻³ |
| 890 | < 10⁻³ |
| 900 | < 10⁻³ |
| 910 | < 10⁻³ |
| 920 | < 10⁻³ |
| 930 | < 10⁻³ |
| 940 | < 10⁻³ |
| 950 | < 10⁻³ |
| 960 | < 10⁻³ |
| 970 | < 10⁻³ |
| 980 | < 10⁻³ |
| 990 | < 10⁻³ |
| 1,000 | < 10⁻³ |
| 1,010 | < 10⁻³ |
| 1,020 | < 10⁻³ |
| 1,030 | < 10⁻³ |
| 1,040 | < 10⁻³ |
| 1,050 | < 10⁻³ |
| 1,060 | < 10⁻³ |
| 1,070 | < 10⁻³ |
| 1,080 | < 10⁻³ |
| 1,090 | < 10⁻³ |
| λ [nm] | |
|---|---|
| 1,100 | < 10⁻³ |
| 1,110 | < 10⁻³ |
| 1,120 | 0.001 |
| 1,130 | 0.001 |
| 1,140 | 0.002 |
| 1,150 | 0.002 |
| 1,160 | 0.003 |
| 1,170 | 0.003 |
| 1,180 | 0.004 |
| 1,190 | 0.005 |
| 1,200 | 0.006 |
| 1,250 | 0.014 |
| 1,300 | 0.029 |
| 1,350 | 0.056 |
| 1,400 | 0.095 |
| 1,450 | 0.147 |
| 1,500 | 0.210 |
| 1,550 | 0.281 |
| 1,600 | 0.356 |
| 1,650 | 0.433 |
| 1,700 | 0.504 |
| 1,750 | 0.570 |
| 1,800 | 0.628 |
| 1,850 | 0.681 |
| 1,900 | 0.728 |
| 1,950 | 0.761 |
| 2,000 | 0.794 |
| 2,050 | 0.821 |
| 2,100 | 0.846 |
| 2,150 | 0.862 |
| λ [nm] | |
|---|---|
| 2,200 | 0.876 |
| 2,250 | 0.886 |
| 2,300 | 0.901 |
| 2,350 | 0.908 |
| 2,400 | 0.914 |
| 2,450 | 0.921 |
| 2,500 | 0.920 |
| 2,550 | 0.921 |
| 2,600 | 0.921 |
| 2,650 | 0.920 |
| 2,700 | 0.917 |
| 2,750 | 0.906 |
| 2,800 | 0.863 |
| 2,850 | 0.785 |
| 2,900 | 0.712 |
| 2,950 | 0.655 |
| 3,000 | 0.607 |
| 3,050 | 0.564 |
| 3,100 | 0.522 |
| 3,150 | 0.483 |
| 3,200 | 0.448 |
| 3,250 | 0.417 |
| 3,300 | 0.392 |
| 3,350 | 0.371 |
| 3,400 | 0.356 |
| 3,450 | 0.346 |
| 3,500 | 0.342 |
| 3,550 | 0.345 |
| 3,600 | 0.352 |
| 3,650 | 0.366 |
| λ [nm] | |
|---|---|
| 3,700 | 0.384 |
| 3,750 | 0.400 |
| 3,800 | 0.402 |
| 3,850 | 0.375 |
| 3,900 | 0.330 |
| 3,950 | 0.278 |
| 4,000 | 0.215 |
| 4,050 | 0.139 |
| 4,100 | 0.078 |
| 4,150 | 0.042 |
| 4,200 | 0.023 |
| 4,250 | 0.015 |
| 4,300 | 0.014 |
| 4,350 | 0.014 |
| 4,400 | 0.013 |
| 4,450 | 0.011 |
| 4,500 | 0.008 |
| 4,550 | 0.007 |
| 4,600 | 0.007 |
| 4,650 | 0.009 |
| 4,700 | 0.014 |
| 4,750 | 0.022 |
| 4,800 | 0.034 |
| 4,850 | 0.047 |
| 4,900 | 0.063 |
| 4,950 | 0.085 |
| 5,000 | 0.110 |
| 5,050 | 0.133 |
| 5,100 | 0.151 |
| 5,150 | 0.158 |
光学值
| 反射系数 | |
|---|---|
| Pd | 0.914 |
| 参考厚度 | |
|---|---|
| d [mm] | 1 |
| 承诺光谱值 | |
|---|---|
| τi (405nm) | ≥0.8 |
| τi (514nm) | ≥0.9 |
| τi (633nm) | ≥0.08 |
| τi (694nm) | ≤0.004 |
| τi (1060nm) | ≤0.0005 |
| 折射率 n |
|---|
| nF (486.1 nm) = 1.546 |
| nh (404.7 nm) = 1.554 |
| ng (435.8 nm) = 1.550 |
| ns (852.1 nm) = 1.533 |
| ne (546.1 nm) = 1.542 |
| nd (587.6 nm) = 1.540 |
色度评估
| 光源 | A(Planck T = 2347K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.317 | 0.252 | 0.215 |
| y | 0.438 | 0.438 | 0.430 |
| Y | 52 | 37 | 28 |
| λd [nm] | 499 | 497 | 496 |
| Pe | 0.30 | 0.45 | 0.54 |
| 光源 | Planck T = 3200 K | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.298 | 0.238 | 0.205 |
| y | 0.418 | 0.413 | 0.403 |
| Y | 54 | 39 | 30 |
| λd [nm] | 497 | 496 | 495 |
| Pe | 0.31 | 0.46 | 0.55 |
| 光源 | D65 (TC = 6504 K) | ||
|---|---|---|---|
| d [mm] | 1 | 2 | 3 |
| x | 0.226 | 0.191 | 0.172 |
| y | 0.314 | 0.299 | 0.288 |
| Y | 61 | 47 | 38 |
| λd [nm] | 489 | 489 | 488 |
| Pe | 0.33 | 0.47 | 0.55 |
物理值
| 密度 | |
|---|---|
| p [g/cm3] | 2.848 |
| 气泡含量 | |
|---|---|
| 气泡等级 | |
| 玻转温度 | |
|---|---|
| Tg [°C] | 410 |
| 温度系数 | |
|---|---|
| Tk [nm/°C] | |
| 耐化学性 | |
|---|---|
| 耐污性 | 1 |
| 耐酸性 | 52.3 |
| 耐碱性 | 3.3 |
| 热膨胀 | |
|---|---|
| α-30°C/+70°C [10-6/K] | 11.79 |
| α20°C/300°C [10-6/K] | 13.65 |
| α20°C/200°C [10-6/K] | |