玻璃类型 |
物品编号 |
长度 |
宽度 |
厚度 |
重量 |
---|
NG9

- SCHOTT
- NG9 - NG9
- 厚度
- 1.0
- 反射系数
- 0.9207
λ [nm] | |
---|---|
200 | < 10⁻³ |
210 | < 10⁻³ |
220 | < 10⁻³ |
230 | < 10⁻³ |
240 | < 10⁻³ |
250 | < 10⁻³ |
260 | < 10⁻³ |
270 | < 10⁻³ |
280 | < 10⁻³ |
290 | < 10⁻³ |
300 | < 10⁻³ |
310 | < 10⁻³ |
320 | < 10⁻³ |
330 | < 10⁻³ |
340 | < 10⁻³ |
350 | < 10⁻³ |
360 | < 10⁻³ |
370 | 0.003 |
380 | 0.005 |
390 | 0.015 |
400 | 0.023 |
410 | 0.028 |
420 | 0.031 |
430 | 0.034 |
440 | 0.036 |
450 | 0.039 |
460 | 0.043 |
470 | 0.044 |
480 | 0.042 |
490 | 0.041 |
λ [nm] | |
---|---|
500 | 0.040 |
510 | 0.039 |
520 | 0.039 |
530 | 0.040 |
540 | 0.041 |
550 | 0.042 |
560 | 0.041 |
570 | 0.040 |
580 | 0.039 |
590 | 0.039 |
600 | 0.041 |
610 | 0.043 |
620 | 0.045 |
630 | 0.047 |
640 | 0.049 |
650 | 0.052 |
660 | 0.055 |
670 | 0.062 |
680 | 0.070 |
690 | 0.081 |
700 | 0.091 |
710 | 0.100 |
720 | 0.107 |
730 | 0.113 |
740 | 0.119 |
750 | 0.123 |
760 | 0.127 |
770 | 0.130 |
780 | 0.132 |
790 | 0.134 |
λ [nm] | |
---|---|
800 | 0.136 |
810 | 0.137 |
820 | 0.138 |
830 | 0.138 |
840 | 0.138 |
850 | 0.137 |
860 | 0.135 |
870 | 0.133 |
880 | 0.133 |
890 | 0.132 |
900 | 0.132 |
910 | 0.131 |
920 | 0.129 |
930 | 0.128 |
940 | 0.128 |
950 | 0.127 |
960 | 0.125 |
970 | 0.123 |
980 | 0.123 |
990 | 0.123 |
1,000 | 0.123 |
1,010 | 0.123 |
1,020 | 0.123 |
1,030 | 0.122 |
1,040 | 0.121 |
1,050 | 0.121 |
1,060 | 0.121 |
1,070 | 0.122 |
1,080 | 0.123 |
1,090 | 0.124 |
λ [nm] | |
---|---|
1,100 | 0.125 |
1,110 | 0.127 |
1,120 | 0.130 |
1,130 | 0.132 |
1,140 | 0.134 |
1,150 | 0.136 |
1,160 | 0.139 |
1,170 | 0.141 |
1,180 | 0.144 |
1,190 | 0.147 |
1,200 | 0.150 |
1,250 | 0.169 |
1,300 | 0.198 |
1,350 | 0.227 |
1,400 | 0.254 |
1,450 | 0.281 |
1,500 | 0.306 |
1,550 | 0.322 |
1,600 | 0.327 |
1,650 | 0.329 |
1,700 | 0.330 |
1,750 | 0.330 |
1,800 | 0.332 |
1,850 | 0.337 |
1,900 | 0.347 |
1,950 | 0.358 |
2,000 | 0.370 |
2,050 | 0.385 |
2,100 | 0.400 |
2,150 | 0.414 |
λ [nm] | |
---|---|
2,200 | 0.430 |
2,250 | 0.444 |
2,300 | 0.460 |
2,350 | 0.473 |
2,400 | 0.486 |
2,450 | 0.498 |
2,500 | 0.512 |
2,550 | 0.526 |
2,600 | 0.534 |
2,650 | 0.535 |
2,700 | 0.500 |
2,750 | 0.271 |
2,800 | 0.150 |
2,850 | 0.140 |
2,900 | 0.151 |
2,950 | 0.170 |
3,000 | 0.190 |
3,050 | 0.211 |
3,100 | 0.235 |
3,150 | 0.258 |
3,200 | 0.280 |
3,250 | 0.304 |
3,300 | 0.315 |
3,350 | 0.292 |
3,400 | 0.250 |
3,450 | 0.190 |
3,500 | 0.130 |
3,550 | 0.088 |
3,600 | 0.060 |
3,650 | 0.051 |
λ [nm] | |
---|---|
3,700 | 0.060 |
3,750 | 0.081 |
3,800 | 0.106 |
3,850 | 0.123 |
3,900 | 0.118 |
3,950 | 0.099 |
4,000 | 0.080 |
4,050 | 0.078 |
4,100 | 0.080 |
4,150 | 0.086 |
4,200 | 0.086 |
4,250 | 0.084 |
4,300 | 0.065 |
4,350 | 0.050 |
4,400 | 0.037 |
4,450 | 0.026 |
4,500 | 0.016 |
4,550 | 0.010 |
4,600 | 0.006 |
4,650 | 0.004 |
4,700 | 0.002 |
4,750 | 0.001 |
4,800 | < 10⁻³ |
4,850 | < 10⁻³ |
4,900 | < 10⁻³ |
4,950 | < 10⁻³ |
5,000 | < 10⁻³ |
5,050 | < 10⁻³ |
5,100 | < 10⁻³ |
5,150 | < 10⁻³ |
反射系数 | |
---|---|
Pd | 0.921 |
参考厚度 | |
---|---|
d [mm] | 1 |
承诺光谱值 | |
---|---|
τi (405nm) | =0.025± 0,01 |
τi (546nm) | =0.04± 0,02 |
τi (694nm) | =0.08± 0,02 |
折射率 n |
---|
nd (587.6 nm) = 1.510 |
色度评估
光源 | A(Planck T = 2347K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | Planck T = 3200 K | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
光源 | D65 (TC = 6504 K) | ||
---|---|---|---|
d [mm] | 1 | 2 | 3 |
x | |||
y | |||
Y | |||
λd [nm] | |||
Pe |
密度 | |
---|---|
p [g/cm3] | 2.45 |
气泡含量 | |
---|---|
气泡等级 | 2 |
玻转温度 | |
---|---|
Tg [°C] | 470 |
温度系数 | |
---|---|
Tk [nm/°C] |
耐化学性 | |
---|---|
耐污性 | 1 |
耐酸性 | 3.2 |
耐碱性 | 2.0 |
热膨胀 | |
---|---|
α-30°C/+70°C [10-6/K] | 6.4 |
α20°C/300°C [10-6/K] | 7.2 |
α20°C/200°C [10-6/K] |