Product Variants of Optical Glass
High Homogeneity Glass
                            
                        CHARACTERISTICS
SCHOTT manufactures high-quality glasses up to the homogeneity level H5 in one, two or even three dimensions. All products are supplied with individual test certificates. The homogeneity of our glasses are measured using extremely accurate, highly advanced interferometers. Large apertures (up to 1500 mm) are measured with stitching technology.
YOUR ADVANTAGES
- Glasses of this quality allow extremely high resolution imaging.
 - Short lead times for a wide range of preferred glasses up to the quality level H5 in 1D, 2D or even 3D.
 - Glasses manufactured to the customer’s specified homogeneity level.
 - Homogeneity also available for large castings e.g. SCHOTT N-BK7® with 1000 mm diameter and 250 mm in thickness in H3.
 
i-Line Glass
                            
                        CHARACTERISTICS
i-Line glasses are optical glass types named after the i-wavelength, which offers both high UV-transmittance at 365 nm and a high refractive index homogeneity. These glass types, such as N-BK7HTi, FK5HTi, LF5HTi and LLF1Hti, are available in both customized shapes and as a final component. i-Line glasses can typically be found in lithography applications such as i-line steppers and wafer scanners.
YOUR ADVANTAGES
- Negligible stress birefringence due to a well-defined annealing process.
 - Excellent internal quality.
 - Availability of a wide range of high transmission glass types, providing high levels of flexibility in optical design.
 
HT and HTultra Glass
                            
                        CHARACTERISTICS
Meanwhile, as DSLR camera and Ultra HD TV grow in popularity, SCHOTT’s HT and HTUltra optical glass can also play a key role in those fields. Offering improved color contribution and better mesopic vision, as well as faster polymerization of UV active glues due to better UV transmittance, it’s a versatile and high-performance range.
YOUR ADVANTAGES
- Improved transmittance especially at the blue-violet spectral range.
 - Reduced thermal lensing effect due to higher transmittance.
 - Reduced energy absorption so improved image quality.
 
Low Tg Glass for Precision Molding
                            
                        CHARACTERISTICS
Precision molding is used for the volume production of complex lenses, with SCHOTT’s range of Low Tg glasses including P-SF68, P-SK57Q1, P-SK58A and P-BK7. The composition of these glasses decreases the tendency for devitrification and reduces the reaction with mold materials within the molding temperature range.
YOUR ADVANTAGES
- Tight optical tolerance.
 - Wide range of dimensions.
 - Available in the form of optical glass rods and ball lenses in different formats.
 
Radiation Resistant Glass
CHARACTERISTICS
SCHOTT offers a variety of specialty radiation resistant glasses that protects against the harmful effects of radiation. By adding cerium to the composition, optical glass can be stabilized against transmittance loss caused by ionizing radiation. The added cerium means the color of these glasses are slightly different from our other products, displaying a yellowish tint, while the UV-transmittance edge is shifted to a longer wavelength.
YOUR ADVANTAGES
- High homogeneity and internal quality.
 - Suitable for earth orbit-based applications with lifetimes of up to 10 years.
 - Polishable and coatable, radiation resistant glass also comes in the form of cut blanks, pressings and rods, as well as finished optical components.