Optical analytics
Typical questions
- Determination of refractive index and dispersion
- Determination of spectral transmission
Methods in detail
Refractive index and dispersion with precision accuracy (prism method)
Procedures
Calculation of spectral refractive indices from
- Measured values of the refractive angle of the prism
- Measured values of the angles of spectral minimum deviation at the prism
Applications
- Determination of the refractive index for transparent materials, which typically are in a refractive index range of 1.4 ≤ nd ≤ 2.2.
- Accuracy >4*10^-6
Refractive index and dispersion with high accuracy (V-block method)
Procedures
Light from spectral lamps is refracted at media boundaries. The spectral refractive indices are calculated from the angles of spectral light deflection.Applications
- Determination of the refractive index or dispersion of optical glass, colored glass, and glass ceramics.
- The wavelength range is between 365 nm and 1014 nm.
- Accuracy >2*10 ^-5
Refractive index and dispersion using prism coupler refractography with standard accuracy
Procedures
Optical modes are generated in the boundary area between the test specimen and the coupling prism using a laser beam. Their spectral, angle-dependent reflection is measured, and the refractive index is calculated from this.Applications
Determination of the refractive index or dispersion between 1.3 and 2.5 for
- Transparent and colored glasses
- Glass ceramics
- and polymers
in the wavelength range from 400 nm to 1550 nm
- Accuracy: >3*10-4
Determination of spectral transmittance
Procedures
Determination of spectral transmission using a dual-beam UV/VIS/NIR spectrophotometer.Applications
Determination of transmission on test specimens made of
- glass
- glass ceramics
- and other light-transmitting materials
in the spectral range from 250 nm to 20.000 nm
Our methods of optical analysis
- Determination and application of optical properties using spectroscopy (UV to IR) for transmission, reflection, and diffuse reflection (remission), in some cases at various sample temperatures up to 700°C (accredited)
- Measurement of fluorescence properties (excitation, emission, quantum yield, and decay time), in some cases at various sample temperatures up to 500°C (accredited)
- Refractive index determination on bulk glass and coatings using prism couplers and ellipsometry for a wavelength range of 400–1600 nm (accredited)
- Performing radiation-induced changes (solarization) and identifying their causes regarding discoloration and scattering (accredited)
- Optical stress analysis of chemically and thermally tempered glass (accredited)
- Determination of the stress-optical coefficient (SOK), measurement of stress birefringence and body stress of glass (accredited)
- Special optical measurement technology according to customer requirements
Highlights
Our approach
Our experts at SCHOTT Analytics look forward to hearing from you. Together with you, our experts will develop the best solution for your needs.