Product Variants of NEXTREMA®
NEXTREMA® transparent
                            
                        Temperature shock resistant, infrared-permeable, transparent: this glass all-rounder with clear through-vision has enormous potential in all areas of industrial and product design, and is the material of choice when processes need to be monitored or inner workings made visible – especially at high temperatures.
- Fire and ice? Nothing shocks this glass-ceramic. Temperature shock-resistance up to 820°C¹.
 - A linear thermal glass expansion coefficient of almost zero.
 - Transmits shortwave light, with high transmission in the infrared spectrum.
 
FIELDS OF APPLICATION
- Cover plates for radiant heating elements in industrial processes.
 - Inspection windows for high-temperature processes.
 - Support plates for high-temperature processes.
 - Substrates for transparent thin-layer heating elements.
 
1 Tested by quenching a homogeneously heated NEXTREMA® transparent panel (820°C) with room temperature water (20°C).
NEXTREMA® translucent white
                            
                        This translucent white variant also appeals to designers and engineers, who use its attractive visible light transference in their LED lighting systems to add atmosphere and illumination in areas of industrial and product design.
- Reduction of visible light in combination with high infrared transmission.
 - Almost invincible in the face of acids and bases with outstanding chemical resistance (for details see chemical properties).
 
FIELDS OF APPLICATION
- Glare-reducing covers for radiant heaters.
 - Elegant cover plates for indoor and outdoor heaters.
 - Heat beds for 3D printers.
 
NEXTREMA® opaque white
Alongside outstanding chemical resistance to acids and bases to DIN 12116, ISO 695 and DIN ISO 719 standards allow the homogeneously colored glass-ceramic to withstand even the most demanding conditions. This visually appealing and non-porous glass-ceramic is also used by designers and architects to add a sophisticated touch to a range of designs.
- Able to withstand temperatures of up to 950°C1.
 - Excellent heat insulation thanks to low transmission in the shortwave IR spectrum.
 - Chemically resistant glass-ceramic, even in aggressive environments. Acids, bases and hydrolytic influences according to DIN 12116, ISO 695 und DIN ISO 719 have no impact on this material. For further details see chemical properties.
 
FIELDS OF APPLICATION
- Inner lining for high-temperature cleanroom furnaces.
 - Easy-clean cover plates for magnetrons in microwave ovens.
 - Decorative element for applications in the fields of architecture, furniture and the household appliance industry.
 - Light diffusers for the lighting sector.
 
1 Applies to NEXTREMA® opaque white for 1 hour at 950°C homogenous heating. For inhomogeneous the operating temperature may vary.
NEXTREMA® tinted
                            
                        Other key features are its excellent transmission capacity for infrared radiation and near-zero thermal expansion, making it ideal for indoor and outdoor heaters in both domestic and industrial settings.
- Extraordinary bending strength of up to 80 MPa (for 4 mm thick glass-ceramic).
 - Reduction of visible light in combination with high infrared transmission.
 - Good transmittance for IR radiation.
 - High degree of resistance to temperature shocks and a linear thermal expansion coefficient of almost zero.
 
FIELDS OF APPLICATION
- Attractive covers for indoor and outdoor radiant heaters.
 - Glare-reducing covers for infrared heaters (for example, in industrial drying processes).
 - Decorative element for applications in the fields of architecture, furniture and the household appliance industry.
 
NEXTREMA® translucent bluegrey
                            
                        The material also has an impressive ‘dead-front’ lighting effect – when viewed from the top none of the parts below are visible, yet the light still shines from below. Taken with its attractive color, this translucent, bluegrey glass-ceramic serves as a visual highlight for industrial and product design.
- Reduction of visible light in combination with high infrared transmission.
 - High bending strength.
 - Outstanding translucent design.
 
FIELDS OF APPLICATION
- Elegant cover plates for indoor and outdoor heaters.
 - Decorative element for applications in the fields of architecture, furniture and household appliances.
 
NEXTREMA® opaque grey
                            
                        Able to serve as a decorative element in product design, this special material is also highly heat resistant. This makes it ideal for use in all areas of industrial production, such as display manufacturing, as well as heating appliances and microwaves.
- Opaque material that blocks visible light.
 - Strong heat-insulation properties due to low overall transmission in the IR spectrum.
 - Opaque glass-ceramic with outstanding temperature resistance.
 - Chemically resistant to acids and bases, and corrosion-resistant special glass according to DIN 12116, ISO 695 and DIN ISO 719 (for details see chemical properties).
 
FIELDS OF APPLICATION
- Inner lining of high-temperature cleanroom furnaces (e.g. display manufacturing).
 - Easy-clean cover plates for magnetrons in microwave ovens.
 - Decorative cover plates for dark radiator heating systems.
 
Specifications and processing
The current status of availability by material and form of delivery has to be requested by the customer. Not all combinations are producible. Other forms of delivery are available on request.
General appearance
Transparent, translucent white, opaque white, tinted, translucent bluegrey and opaque grey. One side with nubs available on request. Grooved surface for tinted, translucent bluegrey and opaque grey on request.
| 
             Thickness  | 
            
             Standard length  | 
            
             Standard width  | 
        
|---|---|---|
| 
             3 mm  | 
            
             50 - 1930 mm  | 
            
             50 - 1075 mm  | 
        
| 
             4 mm  | 
            
             50 - 1930 mm  | 
            
             50 - 1075 mm  | 
        
| 
             5 mm  | 
            
             50 - 1930 mm  | 
            
             50 - 1075 mm  | 
        
| 
             6 mm  | 
            
             50 - 1930 mm  | 
            
             50 - 1075 mm  | 
        
With regard to the specific format of all the following characteristics, please refer to the net-size, as agreed upon with the customer. Other forms of delivery are available on request.
| 
             Characteristics / Areas / Location  | 
            
             Tolerance  | 
        |
|---|---|---|
| 
             Thickness t  | 
            
             t = 3.0 / 4.0 / 5.0 mm  | 
            
             ± 0.2 mm  | 
        
| 
             t = 6.0 mm  | 
            
             ± 0.3 mm  | 
        |
| 
             Edge length l  | 
            
             l ≤ 500 mm  | 
            
             ± 1.0 mm  | 
        
| 
             l > 500 mm  | 
            
             ± 1.5 mm  | 
        |
| 
             Squareness (ISO 1101) (depending on the edge length l)  | 
            
             l ≤ 500 mm  | 
            
             ≤ 1.0 mm  | 
        
| 
             l > 500 mm  | 
            
             ≤ 1.5 mm  | 
        |
| 
             Flatness along the diagonal D (depending on edge length l)  | 
            
             l ≤ 300 mm  | 
            
             ≤ 0.3 mm  | 
        
| 
             l > 300 mm  | 
            
             Max. 0.3% x D  | 
        |
| 
             Corner radius r  | 
            
             r ≤ 5 mm  | 
            
             ± 5.0 mm  | 
        
| 
             5 mm < r ≤ 20 mm  | 
            
             ± 1.0 mm  | 
        |
| 
             r > 20 mm  | 
            
             ± 2.0 mm  | 
        |
| 
             Drilled holes  | 
            
             Diameter of drilled holes  | 
            
             Max. ± 1.0 mm  | 
        
| 
             Borehole position to reference  | 
            
             ± 1.5 mm  | 
        

Various formats and shapes of bent panels, as well as further data and information, are available on request. Please do not hesitate to contact us.