SCHOTT compressor terminals have excellent pressure resistance and are used as feedthroughs for electrical supply to compressors. SCHOTT develops and manufactures compressor terminals using hermetic compression glass-to-metal sealing, delivering high mechanical strength and electrical insulation. They are designed to perform reliably in extreme environmental conditions.
Features of SCHOTT compressor terminals
Compressor Terminals for Refrigeration & Air Conditioning

Automotive Air Conditioning Compressor Terminals
| Voltage | Electric Current | Pin Material | Pim Diameter (mm) | Insulation Material (Rubber) | Insulation Material (Ceramic) |
|---|---|---|---|---|---|
| 24 V - 48 V | 80 A - 150 A | Cr-Cu | 4.0 - 6.0 | Optional | Optional |
| 200 V - 500 V | Up to 30 A | Fe-Cr | 3.2 | Optional | Optional |
| 200 V - 500 V | 30 A - 50 A | Cu plated Fe-Cr | 3.2 | Optional | Optional |
| 800 V | Up to 30 A | Fe-Cr | 3.2 | Yes | Yes |
| 800 V | 30 A - 50 A | Cu plated Fe-Cr | 3.2 | Yes | Yes |