SCHOTT compressor terminals are used in variety of compressor applications. Our compressor terminals are designed to fulfill unique challenges and requirements for customers, enabling long-term reliability in end-use applications.
Automotive AC e-Compressor Terminals
CHARACTERISTICS
We design and develop compressor terminals by working with electric compressor manufacturers and automotive OEMs worldwide. Based on many years of compressor and automotive sector experience, SCHOTT can offer fully performance-optimized standard products, as well as custom-made automotive air conditioning compressor terminals that fulfill even the most challenging requirements.
YOUR ADVANTAGES
- High voltage capability: 800 V.
- High current capability: 30-150 A (required for 48 V technology).
- High pressure resistance: 20 MPa (required for CO2 refrigerants).
Compressor Terminals for Refrigeration and Air Conditioning
YOUR ADVANTAGES
- High pressure resistance.
- High voltage capacity.
- Increased insulation using ceramic or rubber as insulation material.
- Broad product line from standard to custom-made options.
CO₂ Compressor Terminals
CHARACTERISTICS
SCHOTT manufactures select CO2 compressor terminals that are designed to withstand these high pressure conditions. Our specialized glass-to-metal sealing process is optimized to maintain hermeticity of CO2 compressors.
YOUR ADVANTAGES
- Pressure-resistant design.
- Special glass with excellent electrical insulation properties.
Semi-Hermetic Screw Compressor Terminals
CHARACTERISTICS
Typical applications for semi-hermetic compressors are in industrial refrigeration: in a supermarket, for example, the doors of a cooled display case are constantly opened and closed. Semi-hermetic compressors enable highly-calibrated refrigeration in environments where temperatures may change frequently. Higher current and voltage than typical refrigeration and air conditioning compressors are required in this application. SCHOTT offers large-scale feedthroughs for these uses.
YOUR ADVANTAGES
- High current capacity.
- Further increase in insulation by using rubber or phenol resin block as insulation material is possible.