N-LASF9HT

玻璃代码:  850322.441

"N"型环保玻璃替代传统的含铅和 砷的玻璃类型。

高透过率玻璃和超高透过率玻璃 - 透射性能更优,尤其是在蓝紫光谱范围内。

在下面的标签或我们的 网页上查找更多的信息。

我们目前可用的玻璃系列采用阿贝图表示, : 交互式阿贝图作为主要工具帮助您选择最合适玻璃。

optical glass klein 4zu3.jpg
特性
nd 1.85025 νd 32.17
ne 1.85650 νe 31.93
nF-nC 0.026430 nF'-nC' 0.026827
您需要帮助或报价吗?
与我们的支持团队联系
技术规格
折射率
特性 λ [nm]
n2,325.4 2,325.4 1.80058
n1,970.1 1,970.1 1.80659
n1,529.6 1,529.6 1.81364
n1,060.0 1,060.0 1.82293
nt 1,014.0 1.82420
ns 852.1 1.82997
nr 706.5 1.83834
nC 656.3 1.84255
nC' 643.8 1.84376
特性 λ [nm]
n632.8 632.8 1.84489
nD 589.3 1.85002
nd 587.6 1.85025
ne 546.1 1.85650
nF 486.1 1.86898
nF' 480.0 1.87058
ng 435.8 1.88467
nh 404.7 1.89845
ni 365.0
特性 λ [nm]
n334.1 334.1
n312.6 312.6
n296.7 296.7
n280.4 280.4
n248.3 248.3
内部透射率
特性 λ [nm]
τ25/2500 2,500 0.598
τ25/2325 2,325 0.712
τ25/1970 1,970 0.919
τ25/1530 1,530 0.986
τ25/1060 1,060 0.994
τ25/700 700 0.986
τ25/660 660 0.981
τ25/620 620 0.979
τ25/580 580 0.978
τ25/546 546 0.972
τ25/500 500 0.945
τ25/460 460 0.898
τ25/436 436 0.855
τ25/420 420 0.801
τ25/405 405 0.703
τ25/400 400 0.653
τ25/390 390 0.513
τ25/380 380 0.314
τ25/370 370 0.095
τ25/365 365 0.030
τ25/350 350
τ25/334 334
τ25/320 320
τ25/310 310
τ25/300 300
τ25/290 290
τ25/280 280
τ25/270 270
τ25/260 260
τ25/250 250
特性 λ [nm]
τ10/2500 2,500 0.814
τ10/2325 2,325 0.873
τ10/1970 1,970 0.967
τ10/1530 1,530 0.994
τ10/1060 1,060 0.998
τ10/700 700 0.994
τ10/660 660 0.992
τ10/620 620 0.992
τ10/580 580 0.991
τ10/546 546 0.989
τ10/500 500 0.978
τ10/460 460 0.958
τ10/436 436 0.939
τ10/420 420 0.915
τ10/405 405 0.869
τ10/400 400 0.843
τ10/390 390 0.766
τ10/380 380 0.629
τ10/370 370 0.390
τ10/365 365 0.246
τ10/350 350 0.005
τ10/334 334
τ10/320 320
τ10/310 310
τ10/300 300
τ10/290 290
τ10/280 280
τ10/270 270
τ10/260 260
τ10/250 250
部分色散
特性
Ps,t 0.2181
PC,s 0.4762
Pd,C 0.2912
Pe,d 0.2366
Pg,F 0.5934
Pi,h
P's,t 0.2149
P'C',s 0.5140
P'd,C' 0.2420
P'e,d 0.2330
P'g,F' 0.5250
P'i,h
特性
ΔPC,t -0.0032
ΔPC,s -0.0016
ΔPF,e 0.0008
ΔPg,F 0.0037
ΔPi,g