SCHOTT Electronic Packaging endeavors to provide reliable, high quality products.


Glass-to-Metal and Ceramic-to-Metal Seals

Hermetically sealed products from SCHOTT Electronic Packaging undergo vigorous testing and quality assurance programs to ensure the high quality our customers expect from SCHOTT products. These processes include test procedures according to MIL STD 883, MIL PRF 38534 JEDEC 9 and Telcordia, such as:
  • Hermeticity
  • Electrical insulation
  • Lead fatigue
  • Visual and dimensional examination
  • Solderability
  • Thermal shock

Large-scale Feedthroughs

During production and at final inspection, each large-scale feedthrough is examined carefully to ascertain pressure stability and hermeticity as well as electrical performance.

Examples of standard quality assurance checks include:
  • Helium leak check (mass spectrometer)
  • Pressure test
  • Electrical tests (high pot and insulation resistance)
  • Visual and dimensional inspection
To qualify new designs, the designs are subject to intensive testing programs which may - depending on the application – additionally include:
  • Cryogenic shock
  • Temperature cyclin
  • Voltage surge
  • Thermal and radiological aging
  • LOCA test
  • Heating under electrical load

Glass Powder

Glass powder from the SCHOTT Group is specially tailored to customer requirements. Depending on the end application, the following quality assurance tests can be conducted:
  • Chemical purity
  • Grain size
  • Tg acc. DIN-ISO 7884
  • α(20-300)
  • Softening point
  • Color

Thermal Cutoffs

Thermal cutoff products undergo vigorous testing and quality assurance processes to ensure stable and reliable quality. In the quality assurance process, we evaluate the operating temperature with tests such as:
  • High temperature test
  • High humidity test
  • Temperature cycle test

Precision Glass Tubes

Precision glass tubes for the encapsulation of electronic components must meet stringent requirements as they are used in special applications such as switches, lamps, identification systems, etc…

Depending on the end use, the following tests can be conducted to assure quality:
  • Dimensional inspection
  • Cleanliness of dust and particles
  • Purity of the glass used
  • Biocompatibility (for animal ID-systems)

Precision Discs

SCHOTT manufactures precision discs of brittle materials such as glass, ceramic, sapphire, etc… for electronic and special applications.

All products must pass a final inspection test for:
  • Dimensional inspection
  • Cleanliness of dust and particles
  • Surface and edge quality (if applicable)
  • Purity of glass used




业务联系

肖特(上海)精密材料和设备国际贸易有限公司

上海市虹梅路1801号凯科国际大厦301室

邮编: 200233 上海市
China
 +86 21 33678000
 +86 21 33678080
电子邮件
Directions
更多联系方式
公司新闻
更多新闻
贸易展览会与活动

06.03 - 08.03.2012

OFC (Optical Fiber Conference)

Los Angeles

13.03 - 15.03.2012

Medtec 2012

Stuttgart

17.04 - 19.04.2012

in-cosmetic

Barcelona

更多贸易展览会