4th Otto Schott Research Award

Anne-Jans Faber, TNO Institute of Applied Physics and Glass Technology, The Netherlands
Erik Muysenberg, TNO Institute of Applied Physics and Glass Technology, The Netherlands
Frank Simonis, TNO Institute of Applied Physics andGlass Technology, The Netherlands
Dr. Ruud Beerkens, TNO Institute of Applied Physics and Glass Technology, The Netherlands

This team worked to develop a mathematical model on simulating the processes in glass melting tanks that would offer the chance of optimizing constructions and process parameters based on detailed experimental investigations.