ILLAX®
- Tubing for ampoules
IL AW15.65±0.12/0.53±0.02 1500 010 200
1639667
产品详情
15.650
+/-
0.120
14.590
0.530
+/-
0.020
1,500.000
94.3
14.5
54
783.0
154
6