CONTURAX® Pro
- Tubing
CD086 BHW 54.75/32.40/1.75 1500 410S
1168584
产品详情
54.750
+/-
0.750
32.400
+/-
0.500
51.250
1.750
+/-
0.150
54.750
+/-
0.750
32.400
+/-
0.500
1,500.000
978.8
14.7
20
294.0
15
5