CONTURAX® Pro
- Tubing
CD085 BW 67,80±1,50/2,75±0,25 1500 310S
1091558
Detalhes do produto
67,800
+/-
1,500
67,800
+/-
1,500
62,300
2,750
+/-
0,250
67,800
+/-
1,500
67,800
+/-
1,500
1.500,000
2.300,0
9,2
35
322,0
4
7