| 001 | unprocessed ends | 
            
                
                    
                        
                        
                            | 002 | cut off and sealed | 
            
                
                    
                        
                        
                            | 003 | cut off and sealed, coated RP40 | 
            
                
                    
                        
                        
                            | 004 | unprocessed and sealed, coated | 
            
                
                    
                        
                        
                            | 005 | unprocessed ends, coated RP40 | 
            
                
                    
                        
                        
                            | 006 | unprocessed and sealed, coated VE-water | 
            
                
                    
                        
                        
                            | 007 | unprocessed ends, coated VE-water | 
            
                
                    
                        
                        
                            | 100 | one end closed, one end slightly fused | 
            
                
                    
                        
                        
                            | 110 | one end closed, one end vial fusing | 
            
                
                    
                        
                        
                            | 111 | one end closed, one end fused | 
            
                
                    
                        
                        
                            | 112 | one end closed, one end heavy toe-in | 
            
                
                    
                        
                        
                            | 113 | one end closed, one end vial fusing, tubing coated | 
            
                
                    
                        
                        
                            | 114 | one end heavy toe-in, one end drawn in | 
            
                
                    
                        
                        
                            | 115 | one end round bottom, one end lightly fused, without gradation | 
            
                
                    
                        
                        
                            | 116 | one end closed with pressure compensation vent, one end vial fusing | 
            
                
                    
                        
                        
                            | 117 | one end closed with pressure compensation vent, one end vial fusing, tubing coated | 
            
                
                    
                        
                        
                            | 120 | one end closed with pressure compensation vent, one end heavily fused, tubing coated | 
            
                
                    
                        
                        
                            | 121 | one end closed with pressure compensation vent, one end normal fused | 
            
                
                    
                        
                        
                            | 122 | one end closed with pressure compensation vent, one end lightly fused, tubing coated | 
            
                
                    
                        
                        
                            | 129 | one end closed with pressure compensation vent, one end heavily drawn in, tubing coated | 
            
                
                    
                        
                        
                            | 130 | one end closed, one end slightly fused, tubing coated | 
            
                
                    
                        
                        
                            | 133 | one end closed, on end heavily fusted, tubing coated | 
            
                
                    
                        
                        
                            | 140 | both ends closed | 
            
                
                    
                        
                        
                            | 143 | both ends closed, coated | 
            
                
                    
                        
                        
                            | 155 | one end round bottom, one end vial fusing, tubing coated | 
            
                
                    
                        
                        
                            | 200 | DENSOCAN®, closed ends | 
            
                
                    
                        
                        
                            | 230 | DENSOCAN®, closed ends, tubing coated | 
            
                
                    
                        
                        
                            | 231 | Ends ground square and parallel | 
            
                
                    
                        
                        
                            | 240 | closed ends, tubing coated with RP40 | 
            
                
                    
                        
                        
                            | 311 | one end slightly fused, one end with vial fusing, coated | 
            
                
                    
                        
                        
                            | 312 | one end slightly fused, one end with vial fusing | 
            
                
                    
                        
                        
                            | 313 | one end with heavy fusing, one end with normal fusing, coated | 
            
                
                    
                        
                        
                            | 314 | one end vial tubing fusing, one end drawn in, coated | 
            
                
                    
                        
                        
                            | 315 | one end vial tubing fusing, one end drawn in | 
            
                
                    
                        
                        
                            | 340 | open ends, tubing coated with RP40, ends coated | 
            
                
                    
                        
                        
                            | 341 | open ends, tubing coated with RP40, ends with normal coating | 
            
                
                    
                        
                        
                            | 342 | light glazed and coated with RP40 | 
            
                
                    
                        
                        
                            | 343 | light glazed and coated with RP40, ends coated | 
            
                
                    
                        
                        
                            | 510 | tubing with AR- coating, ends fused | 
            
                
                    
                        
                        
                            | 600 | slightly fused ends | 
            
                
                    
                        
                        
                            | 610 | ends with normal fusing | 
            
                
                    
                        
                        
                            | 611 | ends with heavy fusing | 
            
                
                    
                        
                        
                            | 613 | one end with heavy fusing, one end with normal fusing | 
            
                
                    
                        
                        
                            | 614 | heavy toe-in | 
            
                
                    
                        
                        
                            | 615 | drawn in ends | 
            
                
                    
                        
                        
                            | 616 | vial fusing | 
            
                
                    
                        
                        
                            | 617 | vial fusing, tubing coated | 
            
                
                    
                        
                        
                            | 618 | one end toe-in, one end heavy toe-in, coated | 
            
                
                    
                        
                        
                            | 619 | Vial tubing fusing, coated RP40 | 
            
                
                    
                        
                        
                            | 625 | ends plain cut | 
            
                
                    
                        
                        
                            | 627 | drawn-in ends, coated RP40 | 
            
                
                    
                        
                        
                            | 628 | heavy toe-in, coated | 
            
                
                    
                        
                        
                            | 629 | drawn in ends, tubing coated | 
            
                
                    
                        
                        
                            | 630 | slightly fused ends, tubing coated | 
            
                
                    
                        
                        
                            | 631 | ends heavily fused, coated tubing | 
            
                
                    
                        
                        
                            | 632 | ends with normal fusing, tubing coated | 
            
                
                    
                        
                        
                            | 633 | one end drawn in, one end heavily fused, tubing coated | 
            
                
                    
                        
                        
                            | 634 | one end drawn in, one end with normal fusing | 
            
                
                    
                        
                        
                            | 635 | one end drawn in, one end heavily fused | 
            
                
                    
                        
                        
                            | 636 | one end slightly fused, one end drawn in, coated | 
            
                
                    
                        
                        
                            | 637 | one end slightly fused, one end heavily fused, coated | 
            
                
                    
                        
                        
                            | 638 | one end slightly fused, one end heavily fused | 
            
                
                    
                        
                        
                            | 641 | ends heavily fused, tubing coated with RP40 | 
            
                
                    
                        
                        
                            | 645 | slightly fused ends, tubing coated | 
            
                
                    
                        
                        
                            | 646 | ends slightly fused, coated RP40 tubing, ends coated | 
            
                
                    
                        
                        
                            | 647 | ends slightly fused, coated tubing, ends coated | 
            
                
                    
                        
                        
                            | 660 | Clearence diameter fusing | 
            
                
                    
                        
                        
                            | 661 | Clearence diameter fusing coated | 
            
                
                    
                        
                        
                            | 662 | Clearence diameter fusing coated with RP 40 |