FIOLAX® clear
- Tubing for vials

FKO AW24.00±0.19/1.00±0.04 1500 010 200
1029690
Product Details
24.000
+/-
0.190
22.000
1.000
+/-
0.040
1,500.000
253.5
16.0
54
864.0
63
6