FIOLAX® amber
 
FBO AW16.00±0.14/1.00±0.04 1500 010 200
1031958
Product Details
16.000 +/- 0.140

14.000

1.000 +/- 0.040

1,500.000

171.3

20.7

54

1,117.8

121