DURAN®

 - Tubing

DURAN®
 
DAW33.00±0.30/2.00±0.09 1500 400 610 V8S
1026072
Product Details
33.000 +/- 0.300

29.000

2.000 +/- 0.090

1,500.000

651.2

16.2

20

324.0

25

5

 
To product list