MIROGARD® Protect

MIROGARD® Protect

SCHOTT MIROGARD® is an anti-reflective, completely transparent glass for use in glazing pictures. The additional versions MIROGARD® Plus and MIROGARD® Protect also provide increased UV protection. It minimizes reflections to less than 1% and provides art lovers with an unrestricted view. The ideal invisible protection.

The dimensions given are usually net dimensions without dipping edge. The gross dimension is supplied including the dipping edge.

Advantages:

  • Anti-reflective coating
  • Splinter protection
  • Outstanding UV protection: 99.9%
  • High mechanical stability
  • Best possible color rendering index of Ra=100
Article T
H
W
sqm.
Sides coated
Reflect. Color
Cont./Box (pcs.)
Cont./Box (sqm.)
General Description

SCHOTT MIROGARD® vs. conventional Float Glass

MIROGARD® glass reduces reflections in the visible spectrum to under 1% and thus allows for an unadulterated view of art.


 MIROGARD®MIROGARD® plusMIROGARD® ProtectMIROGARD® Protect Ultra
Reflectance
ρvA %
~ 0.9%~ 1.1%~ 0.9%~ 0.9%
Transmittance
τvA %
~ 99%~ 98%~ 98%~ 98%
Mechanical protection effectlowlowmedium
to high
medium
to high
Splinter protection
UV Protection
(300 – 380 nm)
~ 48%~ 82%~ 99%~ 99%

Coating durability

SCHOTT makes an enormous technical effort to provide a nearly reflection-free view: MIROGARD® anti-reflective glass is dip-coated using the sol-gel process.

All products have passed the following tests:
- copper chloride acetic acid spray test
- sliding abrasion with Taber Abraser process
- adhesive tape test
- alcohol rubbing test
- stylus test

SCHOTT MIROGARD® - Brochure

Cleaning instructions for coated glass