Forschungsberichte 2006-2007
Zusammensetzung, Eigenschaften und Anwendung von Glaskeramiken
Döhring, T.; Hartmann, P.; Jedamzik, R.; Thomas, A.; Lentes, F.-T.
Properties of Zerodur mirror blanks for extremely large telescopes
AOMATT 2005: 2. International Symposium on Advanced Optical Manufacturing and Testing Technologies, Session 1: Large Mirrors and Telescopes / Zhang, Y.; Jiang, W.; Cho, M.K., eds., Bellingham, WA: SPIE, 2006, article no. 61480G, 8 p. - (Proceedings of SPIE ; 6148)
Properties of Zerodur mirror blanks for extremely large telescopes
AOMATT 2005: 2. International Symposium on Advanced Optical Manufacturing and Testing Technologies, Session 1: Large Mirrors and Telescopes / Zhang, Y.; Jiang, W.; Cho, M.K., eds., Bellingham, WA: SPIE, 2006, article no. 61480G, 8 p. - (Proceedings of SPIE ; 6148)
Döhring, T.; Jedamzik, R.; Hartmann, P.
Mirrors for solar telescopes made from ZERODUR® glass ceramic
Solar Physics and Space Weather Instrumentation II, San Diego, MA / Fineschi, P.; Viereck, R.A., eds., Bellingham, WA: SPIE, 2007. - (Proceedings of SPIE ; 6689)
Mirrors for solar telescopes made from ZERODUR® glass ceramic
Solar Physics and Space Weather Instrumentation II, San Diego, MA / Fineschi, P.; Viereck, R.A., eds., Bellingham, WA: SPIE, 2007. - (Proceedings of SPIE ; 6689)
Döhring, T.; Thomas, A.; Jedamzik, R.; Kohlmann, H.; Hartmann, P.
Manufacturing of lightweighted ZERODUR® components at SCHOTT
Optical Materials and Structures Technologies III, San Diego, CA / Goodman, W.A.; Robichaud, J.L., eds., Bellingham, WA: SPIE, 2007. - (Proceedings of SPIE ; 6666)
Manufacturing of lightweighted ZERODUR® components at SCHOTT
Optical Materials and Structures Technologies III, San Diego, CA / Goodman, W.A.; Robichaud, J.L., eds., Bellingham, WA: SPIE, 2007. - (Proceedings of SPIE ; 6666)
Engel, A.; Letz, M.; Zachau, T.; Pawlowski, E.; Seneschal-Merz, K.; Korb, T.; Enseling, D.; Hoppe, B.; Peuchert, U.; Hayden, J.S.
Reference based optical characterization of glass-ceramic converter for high power white LEDs
Light-Emitting Diodes: Research, Manufacturing, and Applications XI / Streubel, K.P.; Jeon, H., eds., Bellingham, WA: SPIE, 2007, article no. 64860Y, 10 p. - (Proceedings of SPIE ; 6486)
Reference based optical characterization of glass-ceramic converter for high power white LEDs
Light-Emitting Diodes: Research, Manufacturing, and Applications XI / Streubel, K.P.; Jeon, H., eds., Bellingham, WA: SPIE, 2007, article no. 64860Y, 10 p. - (Proceedings of SPIE ; 6486)
Hartmann, P.; Nattermann, K.; Döhring, T.; Kuhr, M.; Thomas, P.; Kling, G.; Gath, P.; Lucarelli, S.
Strength aspects for the design of ZERODUR® glass ceramics structures
Optical Materials and Structures Technologies III, San Diego, CA / Goodman, W.A.; Robichaud, J.L., eds., Bellingham, WA: SPIE, 2007. - (Proceedings of SPIE ; 6666)
Strength aspects for the design of ZERODUR® glass ceramics structures
Optical Materials and Structures Technologies III, San Diego, CA / Goodman, W.A.; Robichaud, J.L., eds., Bellingham, WA: SPIE, 2007. - (Proceedings of SPIE ; 6666)
Jedamzik, R.; Hartmann, P.
Influence of striae on the homogeneity of the linear thermal expansion coefficient of ZERODUR®
Current Developments in Lens Design and Opcial Engineering VII / Mouroulis, P.Z.; Smith, W.J.; Johnson, R.B., eds., Bellingham, WA: SPIE, 2006, article no. M2880, 12 p.. - (Proceedings of SPIE ; 6288)
Influence of striae on the homogeneity of the linear thermal expansion coefficient of ZERODUR®
Current Developments in Lens Design and Opcial Engineering VII / Mouroulis, P.Z.; Smith, W.J.; Johnson, R.B., eds., Bellingham, WA: SPIE, 2006, article no. M2880, 12 p.. - (Proceedings of SPIE ; 6288)
Jedamzik, R.; Müller, R.; Hartmann, P.
Homogeneity of the linear thermal expansion coefficient of ZERODUR® measured with improved accuracy
Optomechanical Technologies for Astronomy, Parts 1 and 2 / Atad-Ettedgui, E.; Antebi, J.; Lemke, D., eds., Bellingham, WA: SPIE, 2006, article no. 627306, 12 p. - (Proceedings of SPIE ; 6273)
Homogeneity of the linear thermal expansion coefficient of ZERODUR® measured with improved accuracy
Optomechanical Technologies for Astronomy, Parts 1 and 2 / Atad-Ettedgui, E.; Antebi, J.; Lemke, D., eds., Bellingham, WA: SPIE, 2006, article no. 627306, 12 p. - (Proceedings of SPIE ; 6273)