Primoceler performed a Radioisotope leak test with krypton 85 at Oneida Research Center (http://www.orslabs.com/)
The glass packages passed all the tests and so the leak rate is less than 6,0×10-12 atmcm3/s Kr-85.
For the full presentation, please click the link below.