Part Number |
Rated Current (A) |
Rated Voltage (Vdc) |
Breaking Capacity (A) |
Fuse Resistance (mΩ) |
Applicable Series Cell Number |
Applicable Voltage Range (V) |
Heater Resistance (Ω) |
UL | TÜV |
---|---|---|---|---|---|---|---|---|---|
D6SE02–30 | 30 | 80 | 80 | 1.5 ± 0.5 | 1 - 2 | 4.0 ~ 9.6 | 0.90 ± 20% | E357922 | J50247451 |
D6SE03–30 | 3 | 8.4 ~ 19.1 | 4.50 ± 20% | ||||||
D6SE05–30 | 4 - 5 | 10.5 ~ 23.5 | 6.85 ± 20% | ||||||
D6SE09–30 | 6 - 9 | 20.2 ~ 46.3 | 26.00 ± 20% | ||||||
D6SE14–30 | 10 - 14 | 28.0 ~ 62.0 | 50.00 ± 20% | ||||||
D6SE03–45 | 45 | 80 | 120 | 1.4 ± 0.4 | 3 | 9.8 ~ 13.5 | 2.65 ± 20% | E357922 | J50247451 |
D6SE04–45 | 4 | 13.0 ~ 18.4 | 4.65 ± 20% | ||||||
D6SE05–45 | 5 | 16.7 ~ 23.5 | 7.70 ± 20% | ||||||
D6SE07–45 | 6 - 7 | 22.3 ~ 31.5 | 14.40 ± 15% | ||||||
D6SE10–45 | 9 - 10 | 33.0 ~ 46.9 | 31.40 ± 15% | ||||||
D6SE14–45 | 12 - 14 | 43.7 ~ 62.0 | 55.20 ± 15% |