Quality Assurance


SCHOTT Electronic Packaging endeavors to provide reliable, high quality products.


Glass-to-Metal and Ceramic-to-Metal Seals

Hermetically sealed products from SCHOTT Electronic Packaging undergo vigorous testing and quality assurance programs to ensure the high quality our customers expect from SCHOTT products. These processes include test procedures according to MIL STD 883, MIL PRF 38534 JEDEC 9 and Telcordia, such as:
  • Hermeticity
  • Electrical insulation
  • Lead fatigue
  • Visual and dimensional examination
  • Solderability
  • Thermal shock

Large-scale Feedthroughs

During production and at final inspection, each large-scale feedthrough is examined carefully to ascertain pressure stability and hermeticity as well as electrical performance.

Examples of standard quality assurance checks include:
  • Helium leak check (mass spectrometer)
  • Pressure test
  • Electrical tests (high pot and insulation resistance)
  • Visual and dimensional inspection
To qualify new designs, the designs are subject to intensive testing programs which may - depending on the application – additionally include:
  • Cryogenic shock
  • Temperature cyclin
  • Voltage surge
  • Thermal and radiological aging
  • LOCA test
  • Heating under electrical load

Glass Powder

Glass powder from the SCHOTT Group is specially tailored to customer requirements. Depending on the end application, the following quality assurance tests can be conducted:
  • Chemical purity
  • Grain size
  • Tg acc. DIN-ISO 7884
  • α(20-300)
  • Softening point
  • Color

Thermal Cutoffs / Battery Fuses

Thermal cutoff products and battery fuse products undergo vigorous testing and quality assurance processes to ensure stable and reliable quality. In the quality assurance process, we evaluate the operating characteristics with tests such as:
Thermal Cutoffs
  • High temperature test
  • High humidity test
  • Temperature cycle test
Battery Fuses
  • High temperature test
  • High humidity test
  • Board bending test

Precision Glass Tubes

Precision glass tubes for the encapsulation of electronic components must meet stringent requirements as they are used in special applications such as switches, lamps, identification systems, etc…

Depending on the end use, the following tests can be conducted to assure quality:
  • Dimensional inspection
  • Cleanliness of dust and particles
  • Purity of the glass used
  • Biocompatibility (for animal ID-systems)

Precision Discs

SCHOTT manufactures precision discs of brittle materials such as glass, ceramic, sapphire, etc… for electronic and special applications.

All products must pass a final inspection test for:
  • Dimensional inspection
  • Cleanliness of dust and particles
  • Surface and edge quality (if applicable)
  • Purity of glass used
Trade Fairs & Events
01.
September
Trade fair CIOE - China International Optoelectronic Exposition, Shenzhen, China, 01.09 - 03.09.2021
13.
September
Trade fair Gastech, Singapore, Singapore, 13.09 - 16.09.2021
22.
September
Trade fair IDS Internationale Dental-Schau, Köln, Germany, 22.09 - 25.09.2021
25.
January
Trade fair SPIE Photonics West, San Francisco, USA, 25.01 - 27.01.2022
Contact
contact-home.png
SCHOTT AG
Christoph-Dorner-Strasse 29
84028 Landshut
Germany
contact-phone.png
E-Mail to SCHOTT+49 (0)871/826-0