RFID Transponder Glass Capsules

Product Description

SCHOTT VivoTag® transponder glass capsules are used to reliably encapsulate and protect sensitive RFID transponder devices. The main application areas include implantable transponders and bolus transponders for pet and livestock identification and tracking.  


How RFID devices work

RFID stands for "Radio Frequency Identification". RFID transponders consist of a semiconductor chip and an antenna. Using radio waves emitted from a reading unit, specific information can be stored on and read from the chip. The technology functions completely wirelessly: depending on the configuration, the distance between the reading unit and the RFID transponder ranges from several centimeters to as much as one meter. No battery is needed since the necessary energy for sending and receiving is entirely supplied by radio waves from the reading unit.

Biocompatible glass tubes


SCHOTT
VivoTag® transponder glass (also known as 8625) has been successfully used in animal identification for decades, making it the most proven material for implantable RFID applications. As an inert material with consistent chemical stability inside the body, the glass tube enables the required long-term functionality of the electronic components.

SCHOTT’s RFID transponder glass was specially formulated for biocompatibility in animal applications (cytotoxicity, hemo-compatibility).


Small sizes, easy to process

SCHOTT’s RFID transponder glasses are precision-cut glass vials available in customizable dimensions and lengths. The standard outside diameter of such capsules ranges from 1 mm up to 4 mm. Customers can choose the size to achieve an optimal balance between transponder dimensions and required RFID reading distance.

Transponder glasses typically have one sealed and one fire-polished end. Due to the high iron content of the glass, it can be sealed using a variety of light sources (e.g. Nd-Yag lasers).
SCHOTT’s focus on high precision and stable batch-to-batch quality enables our customers to benefit from optimal processability in production.


RFID tracking and identification


Apart from animal identification, VivoTag® glass capsules are also used in technical areas, such as RFID freight tracking and automotive applications, where the RFID transponders need to be reliably protected against harsh environments.



 

Advantages

SCHOTT’s VivoTag® RFID transponder glass offers the following advantages:
 
  • Proven track record SCHOTT‘s 8625 VivoTag® transponder glass has been successfully used in animal identification for decades.
  • Excellent biocompatibility for animal applications demonstrated in various studies.
  • Ease of use in processing and end-use applications thanks to high precision and accuracy in terms of glass composition and dimensional tolerances.
  • Small sizes available down to 1.25 mm outer diameter.
  • Fast and flexible sampling for standard as well as custom-made solutions.
     

Applications

Our customers use SCHOTT VivoTag® transponder glass for the hermetic encapsulation of RFID transponder devices. End-use applications are found in a variety of fields:
 
  • Livestock – the identification and tracking records the origin and supports safety processes for meat
  • Veterinary Industry - biocompatible RFID transponders are subcutaneously injected or implanted with a syringe for pet identification
  • Freight and Automotive Industries: provides logistics support for

 

Technical Details

Technology

The fabrication of glass tubes is one of SCHOTT's key competencies.

All high-precision cutting and sealing equipment has been developed in-house. SCHOTT VivoTag® transponder glass vials have one sealed and one fire-polished end. The fire-polishing of the open end prevents chipping during transportation and eliminates the need for further processing by protecting the electrical unit from damage during insertion into the glass vial.


Features / Specifications

The following table lists all important features of SCHOTT’s RFID transponder glass type 8625:
Properties of transponder glasses VivoTag® 8625
Coefficient of thermal expansion (ISO 7991) α20-300 10-6K-1 9.15
Transformation temperature (ISO 7884-8) °C 514
Temperature at viscosity (ISO 7884-5)104 dPas °C 1023
Density g/cm3 2.52
Young’s Modulus of elasticity GPa 73
Transmission of 0.5 mm glass at 1.1 µm % 15
Classes of chemical stability

water (ISO 719)

acid (DIN 12116)

alkali (ISO 695)
 

3

1

2
Biocompatibility   excellent, tested in animal applications
Please contact us for information about standard and custom dimensions.


Forms of Supply and Product Packaging

VivoTag® transponder glass vials are packaged in antistatic trays or in bags as bulk packaging.

Quality

Please refer to our quality assurance processes page for more information on our various quality assurance programs.
Trade Fairs & Events
04.
September
25.
September
Trade fair Automotive LiDAR 2019, Detroit, MI, USA, 25.09 - 26.09.2019
01.
October
Trade fair European Microwave Week 2019, Paris, France, 01.10 - 03.10.2019
Contact
contact-home.png
SCHOTT AG
Christoph-Dorner-Strasse 29
84028 Landshut
Germany
contact-phone.png
E-Mail to SCHOTT+49 (0)871/826-0
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.