SEFUSE® D6SK Series Data

Dimensions

Dimension (Unit:mm)
D6SC Dimensions

Ratings/Safety Standards

Part
Number
Rated
Current
(A)
Rated
Voltage
(Vdc)
Breaking
Capacity
(A)
Fuse
Resistance
(m
Ω)
Applicable
Series
Cell
Number
Applicable
Voltage
Range
(V)
Heater
Resistance
(
Ω)
UL TÜV
D6SK1–12 12 30 50 3.0 ± 1.0 1 3.5 ~ 4.7 1.20 ± 20% E357922 J50247451
D6SK2–12 2 6.0 ~ 9.2 3.60 ± 15%