SEFUSE® D6SC Series Data

Dimensions

Dimension (Unit:mm)
SEFUSE® D6SC Dimensions

Ratings/Safety Standards

Part Number Rated Current
(A)
Rated Voltage
(Vdc)
Breaking Capacity
(A)
Fuse Resistance 
(mΩ)
Applicable Series Cell Number Applicable Voltage
Range 
(V)
Heater Resistance 
(Ω)
UL TÜV
Made
in Thailand
Made
in Thailand
D6SC1-12 12 36 50 2.0±1.0 3.0 ~ 5.0 1.35±25% E357922 J50247451
D6SC2-12 2 4.0 ~ 9.0 2.50±20%
D6SC3-12 3 7.4 ~ 13.8 8.30±20%
D6SC4-12 4 10.5 ~ 19.6 16.70±20%
D6SC1-15 15 1.5±1.0 1 3.0 ~ 5.0 1.25±20%
D6SC2-15 2 5.0 ~ 9.0 3.20±20%
D6SC3-15 3 7.4 ~ 13.8 6.95±20%
D6SC4-15 4 10.5 ~ 19.6 13.10±20%
D6SC5-15 5 14.4 ~ 23.5 23.50±20%
D6SC6-15 6 16.8 ~ 28.0 36.20±20%
Trade Fairs & Events
27.
April
Trade fair Battery Experts Forum, Frankfurt, Germany, 27.04 - 29.04.2021
13.
September
Trade fair Gastech, Singapore, Singapore, 13.09 - 16.09.2021
Contact
contact-home.png
SCHOTT AG
Christoph-Dorner-Strasse 29
84028 Landshut
Germany
contact-phone.png
E-Mail to SCHOTT+49 (0)871/826-0