SEFUSE® D6SA Series Data

Dimensions

Dimension (Unit:mm)
SEFUSE® D6SA Dimensions

Ratings/Safety Standards

Part Number Rated Current (A) Rated Voltage (Vdc) Breaking Capacity
(A)
Fuse Resistance
(mΩ)
Applicable Series Cell Number Applicable Voltage
Range 
(V)
Heater Resistance
(Ω)
UL TÜV
Made in
Thailand
Made in
Thailand
D6SA2-12 12 36 50 2.0±1.0 1-2 4.0~9.0 2.15±20% E357922 J50247451
D6SA3-12 3 7.4~13.8 7.3±20%
D6SA4-12 4 10.5~19.6 14.7±20%
D6SA3-15 15 1.5±1.0 3 7.4~13.8 6.9±20%
D6SA4-15 4 10.5~19.6 14.0±20%
D6SA5-15 5 14.4~23.5 21.6±20%
D6SA03-30 30 62 80 0.6±0.5 3 9.9~13.5 6.05±20%
D6SA04-30 4 13.4~18.4 11.05±20%
D6SA05-30 5 17.1~23.5 18.0±20%
D6SA06-30 6 20.0~27.5 24.7±20%
D6SA07-30 7 23.0~31.5 32.6±20%
D6SA09-30 9-10 28.0~45.0 60.0±15%
D6SA10-30 9-10 34.2~46.9 75.0±15%
D6SA14-30 13-14 49.0~62.0 154.0±15%
Trade Fairs & Events
16.
November
Trade fair Sensors Expo & Conference, San Jose, CA, USA, 16.11 - 18.11.2020
12.
January
Trade fair European Microwave Week, Utrecht, Netherlands, 12.01 - 14.01.2021
27.
April
Trade fair Battery Experts Forum, Frankfurt, Germany, 27.04 - 29.04.2021
13.
September
Trade fair Gastech, Singapore, Singapore, 13.09 - 16.09.2021
Contact
contact-home.png
SCHOTT AG
Christoph-Dorner-Strasse 29
84028 Landshut
Germany
contact-phone.png
E-Mail to SCHOTT+49 (0)871/826-0