06.04.2016, Munich, Mainz / Germany

Flexible Glass for Printed Electronics

SCHOTT to present flexible glass for use in future applications at LOPEC
Flexible and yet robust: ultra-thin glass from SCHOTT. It can bend to a radius of a few millimeters. Photos: SCHOTT
Flexible and yet robust: ultra-thin glass from SCHOTT. It can bend to a radius of a few millimeters. Photos: SCHOTT
The special glass expert SCHOTT is presenting ultra-thin glasses that enable various functionalities in printed electronic components as a flexible substrate material (Hall B0, Booth 106) at the leading international trade fair for printed and organic electronics LOPEC 2016 from April 6 – 7 in Munich. SCHOTT is also unveiling concepts on how it plans to transfer ultra-thin glass substrates into mass production for applications in organic and printed and organic electronics together with development partners. With respect to the prestigious “Innovation Award of the German Industry”, which will be awarded on April 16, 2016, SCHOTT managed to make it among the four finalists in the category large companies with its ultra-thin glass.

With a minimum thickness of 25 micrometers (microns), these innovative glasses are thinner than a human hair, flexible and yet robust. Thus they offer many advantages over other substrate materials such as plastics, metals or silicon. With properties such as minimum thickness and flexibility that only polymers have offered in the past, the ultra-thin glasses from SCHOTT combine the classic chemical, physical and mechanical advantages of the inorganic material of special glass.

Improved edge strength makes ultra-thin glass more robust and more flexible

SCHOTT is currently the only company in the world that can offer chemically strengthened ultra-thin glass made in a continuous melting process. Due to chemical strengthening, the edge strength is four times higher than glasses that are not treated in this way. This means a significant improvement in the robustness and reliability during further processing and in the final application,” explains Dr. Rüdiger Sprengard, Director New Business Ultra-Thin Glass at SCHOTT AG. “Our ultra-thin glass is an ideal substrate for use in printed electronics. Its high temperature stability enables the sintering of conductive inks. Its unsurpassed hermeticity protects organic materials, which are extremely sensitive to moisture and oxygen. Its excellent optical quality and scratch resistance make it the best choice for the interface to the user,” says Sprengard.

Huge  potential for use in “flexible electronics”

For the application field of organic electronics, SCHOTT is working to build up a manufacturing equipment eco-system together with industry partners. For instance, SCHOTT has been partnering with the adhesives specialist tesa SE, the equipment manufacturer VON ARDENNE GmbH, and the Fraunhofer Institute FEP in the consortial project KONFEKT since 2015. The aim of the project funded by the German BMBF, Federal Ministry of Education and Research, is to refine ultra-thin glass on a roll by laminating it with functional adhesive tapes and by applying special functional layers so that a substrate that is easy to process and offers unique properties can be provided for use in organic electronics.

Various functionalities in printed electronics can be realized using ultra-thin glasses, such as touch sensors, flexible displays, lighting components, solar cells, and smart labels. “This will allow for pioneering innovations in various industries. We are thinking about the areas of consumer electronics, packaging, white goods, and automotive, for example,” says Rüdiger Sprengard.

Initial market successes for ultra-thin glasses

Regardless of the application field in printed electronics, ultra-thin glass from SCHOTT hit the market in November 2015 in first products, such as in the functionality of the cover for fingerprint sensors of high-quality smartphones, improving the authentication reliability of the sensor due to unique material properties of the glass. In the near future, SCHOTT expects to see its ultra-thin glass used in camera modules of smartphones and in semiconductor electronics in the field of chip packaging.

SCHOTT is the only supplier that has five different ultra-thin glasses with various chemical, mechanical, thermal and electrical properties in its portfolio. Thus, the company can provide its customers with a customized product as a sheet, a wafer or wound on a roll, depending on the application.

More information: 
SCHOTT film on ultra-thin glass
https://youtu.be/4XEJKi_ybAw

SCHOTT microsite on ultra-thin glass
https://microsites.schott.com/milestones/english/solutions/irt/ultrathinglass.html?dimsdetected=1&ref=no-referer

SCHOTT is a leading international technology group in the areas of specialty glass and glass-ceramics. The company has more than 130 years of outstanding development, materials and technology expertise and offers a broad portfolio of high-quality products and intelligent solutions. SCHOTT is an innovative enabler for many industries, including the home appliance, pharmaceutical, electronics, optics, automotive and aviation industries. SCHOTT strives to play an important part of everyone’s life and is committed to innovation and sustainable success. The group maintains a global presence with production sites and sales offices in 35 countries. With its workforce of approximately 15,000 employees, sales of 1.93 billion euros were generated in fiscal year 2014/2015. The parent company, SCHOTT AG, has its headquarters in Mainz (Germany) and is solely owned by the Carl Zeiss Foundation. As a foundation company, SCHOTT assumes special responsibility for its employees, society and the environment. www.schott.com

OLED lighting component made of ultra-thin glass from SCHOTT. Photos: SCHOTT
OLED lighting component made of ultra-thin glass from SCHOTT. Photos: SCHOTT
Press contact
SCHOTT AG
Dr. Jürgen Steiner
Public Relations Manager
Hattenbergstraße 10
55122 Mainz
Phone: +49 6131/66-4335
Further information
SCHOTT AG
Salvatore Ruggiero
Vice President Marketing and Communication
Hattenbergstraße 10
55122 Mainz
Phone: +49 6131/66-4140
empty