Location Profile
This facility manufactures special glass tubes and pharmaceutical primary packaging made of glass and polymers.
Facts & Figures
Location (Country): |
Lebanon, PA (USA) |
Number of employees: |
approx. 220 employees |
Founded: |
2003 |
Business Units & Products
Business Units: |
Tubing and Pharmaceutical Systems |
Main products: |
SCHOTT Fiolax®, SCHOTT Boro 8330™ glass tubing for pharmaceutical packaging, SCHOTT Duran® borosilicate tubing, Glass and COC polymer prefillable syringes, glass and COC polymer vials, SCHOTT Type 1 plus® vials, transparent SCHOTT Purgard® containers |