BOROFLOAT® 33 glass is available in the following standard thicknesses and tolerances:
Standard thickness
Thickness (mm)
Tolerance (mm)
0.70 ± 0.05
1.10 ± 0.05
1.75 ± 0.05
2.00 ± 0.05
2.25 ± 0.05
2.75 ± 0.10
3.30 ± 0.20
3.80 ± 0.20
5.00 ± 0.20
5.50 ± 0.20
6.50 ± 0.20
7.50 ± 0.30
9.00 ± 0.30
11.00 ± 0.30
13.00 ± 0.30
15.00 ± 0.40
16.00 ± 0.50
18.00 ± 0.50
19.00 ± 0.50
20.00 ± 0.70
21.00 ± 0.70
25.40 ± 1.00

Panel thickness is continuously measured during production using laser thickness measuring equipment.
Further thicknesses and tolerances are available on request.

Sizes

Please note following stock sizes of BOROFLOAT® 33 glass:
Stock size
Standard size Thickness
1,150 x 850 mm 0.7 – 25.4 mm
1,700 x 1,300 mm 16.0 – 21.0 mm
2,300 x 1,700 mm 0.7 – 15.0 mm


Further data and information available on request.