BOROFLOAT® 33 glass is available in the following standard thicknesses and tolerances:
Standard thickness
Thickness (mm)
Tolerance (mm)
0.70 ± 0.05
1.10 ± 0.05
1.75 ± 0.05
2.00 ± 0.05
2.25 ± 0.05
2.75 ± 0.10
3.30 ± 0.20
3.80 ± 0.20
5.00 ± 0.20
5.50 ± 0.20
6.50 ± 0.20
7.50 ± 0.30
9.00 ± 0.30
11.00 ± 0.30
13.00 ± 0.30
15.00 ± 0.40
16.00 ± 0.50
18.00 ± 0.50
19.00 ± 0.50
20.00 ± 0.70
21.00 ± 0.70
25.40 ± 1.00

Panel thickness is continuously measured during production using laser thickness measuring equipment.
Further thicknesses and tolerances are available on request.

Sizes

Please note following stock sizes of BOROFLOAT® 33 glass:
Stock size
Standard size Thickness
1,150 x 850 mm 0.7 – 25.4 mm
1,700 x 1,300 mm 16.0 – 21.0 mm
2,300 x 1,700 mm 0.7 – 15.0 mm


Further data and information available on request.
Trade Fairs & Events
13.
November
Trade fair electronica, Munich, Germany, 13.11 - 16.11.2018
05.
February
Trade fair SPIE Photonics West, San Francisco, CA, USA, 05.02 - 07.02.2019
SCHOTT uses Cookies on this Website to enhance the user experience and provide the best possible Service. By continuing to browse the Website, you consent to our use of Cookies.

Dear visitor,

we’d like to invite you to participate in our survey regarding the usability of our web presence. Your feedback is important to us and will help us to further improve our information offer.

Please take the opportunity to share your opinion with us. It will only take 5 min of your time.

Thank you very much!
Your SCHOTT Online Team