Thermal tempering

To increase the mechanical and thermal strength of glass, thermal toughening is available for glass thicknesses of around 3 mm or greater. This process involves uniformly heating the glass in an oven to in excess of 600°C and then quickly cooling it with cold air. This creates a compressive pressure zone on the surface of the glass which surrounds a tensile pressure zone within the glass core. The difference in these pressures gives toughened glass a mechanical and thermal strength that is 3–4 times greater than non-tempered glass.

Thermally toughened glass destructs into small glass particles. The glass has specific fracture patterns depending on the grade of thermal tempering. These patterns range from fine particled (tempered safety glass) to coarse and/or dagger-like (heat-strengthened glass).
Ferias y eventos
08.
November
Feria Denkmal, Leipzig, Alemania, 08.11 - 10.11.2018
13.
November
Feria electronica, Munich, Alemania, 13.11 - 16.11.2018
Modificar
SCHOTT utiliza cookies en este sitio web para mejorar la experiencia de uso del mismo y proporcionar el mejor servicio posible. Si continúa navegando por este sitio web, usted estará consintiendo que utilicemos cookies.

Dear visitor,

we’d like to invite you to participate in our survey regarding the usability of our web presence. Your feedback is important to us and will help us to further improve our information offer.

Please take the opportunity to share your opinion with us. It will only take 5 min of your time.

Thank you very much!
Your SCHOTT Online Team