PYRANOVA® for interior applications

empty

At a glance

PYRANOVA® special glass for interior applications is a clear composite or laminated safety glass for use in fire resistant glazing in internal areas that feature fire resistant properties in accordance with DIN EN ISO 12543. Depending on its structure, it is manufactured from at least two float glass panes that contain transparent, fire resistant foaming interlayers.



Design and variety of PYRANOVA®

PYRANOVA® - Butt joint system
PYRANOVA® special glass fits in seamlessly with sophisticated architectural design. The butt joint system with PYRANOVA® special glass, for instance, joins the glass panes together in a frameless manner with the help of a special silicone seal. This allows for the creation of light, smooth sheets of glass that are virtually endless and offer a clear view at all times. PYRANOVA® special glass in the butt joint system also allows for corner constructions.

Technical data

Product Fire
Rating
Thickness Weight Light
Transmission
Ug-Value Sound
Reduction
  acc. EN 13501-2
[mm]
[kg/m2]
[%]
[W/m2K]
[dB]
Interior
PYRANOVA® EW EW 30
7
17
89
5.6
33
PYRANOVA® EW EI 15 / EW 30
11
26
87
5.4
36
PYRANOVA® 30* EI 30
15
35
86
5.1
38
PYRANOVA® 45 EI 45
19
44
85
5
38
PYRANOVA® 60* EI 60
23
55
87
4.8
41
PYRANOVA® 90 EI 90
37
86
84
4.8
44
PYRANOVA® 120 EI 120
52
106
74
2.5
42

*PYRANOVA® Planeline is available for fire rating EI 30
*PYRANOVA® butt jointed glazing is available for fire rating EI 30 and EI 60