Product |
Fire Rating |
Thickness |
Ug-Value |
g-Value |
Light
Transmission |
Sound Reduction |
|
acc. EN 13501-2 |
[mm]
|
[W/m2K]
|
[%]
|
[%]
|
[dB]
|
Heat insulation - Low e coatings |
ISO PYRANOVA® for interior application |
EI (F) 30 |
34
|
1.4
|
54
|
74
|
40
|
EI (F) 30 |
34
|
1.1
|
54
|
74
|
40
|
ISO PYRANOVA® for exterior application |
EI (F) 30 |
38
|
1.4
|
54
|
73
|
40
|
EI (F) 30 |
38
|
1.1
|
54
|
73
|
40
|
ISO PYRANOVA® for interior application |
EI (F) 30 |
30
|
|
|
|
43
|
EI (F) 30 |
37
|
1.4
|
|
|
45
|
Sound insulation |
ISO PYRANOVA® for exterior application |
EI (F) 30 |
42
|
1.4
|
|
|
46
|
EI (F) 30 |
44
|
1.4
|
|
|
47
|
EI (F) 30 |
44
|
1.4
|
|
|
45
|
EI (F) 30 |
54
|
|
|
|
47
|
EI (F) 30 |
52
|
|
|
|
49
|